METHOD FOR FOAMED SLAG GENERATION OF A NON CORROSIVE MELT IN A CONVERTER

机译:转炉中非腐蚀性熔渣的泡沫渣生成方法

摘要

In order to carry out foaming of a slag having a high ratio of chromium oxide having values of often above 20% of a non-corrosive melt in an AOD (Argon Oxygen Decarburization) or MRP (Metallurgical Refining Process) converter or CONARC SSt for stainless steel by adding a foam material, according to the invention a previously defined mixture (5) of a metal oxide, iron carrier, carbon and binding material in the form of pellets or briquettes (4) is introduced into the converter, which reacts in a chemically reducing manner under the slag layer (2) due to the high ambient temperature, wherein gaseous carbon monoxide formed in particular by means of the reduction process of the metal oxide with the carbon within the pellets or briquettes (4) induces the slag foaming with the gas bubbles (7) thereof and wherein the specific density of the pellets or briquettes (4) and the resolve time of the reduction process are selected so that optimal bubble formation in respect of size and duration is achieved. WO2011089027A1
机译:为了在AOD(氩氧脱碳)或MRP(冶金精炼工艺)转炉或CONARC SSt中对高比例氧化铬(其值通常超过非腐蚀性熔体的20%)进行发泡通过加入泡沫材料,根据本发明,将预先定义的由金属氧化物,铁载体,碳和粘结材料制成的颗粒或团块形式的混合物(5)(5)的混合物(5)引入转炉中,在反应器中进行反应。由于高的环境温度而在炉渣层(2)下进行化学还原,其中,特别是通过金属氧化物与球团或团块(4)中的碳的还原过程形成的气态一氧化碳会导致炉渣起泡。选择其气泡(7),其中选择粒料或团块(4)的比重和还原过程的分解时间,以使就尺寸和持续时间而言最佳的气泡形成为ev。 WO2011089027A1

著录项

  • 公开/公告号IN300038B

    专利类型

  • 公开/公告日2018-08-31

    原文格式PDF

  • 申请/专利权人

    申请/专利号IN7021/CHENP/2012

  • 发明设计人 ROSE LUTZ GERMANY;REICHEL JOHANN GERMANY;

    申请日2011-01-05

  • 分类号C21C5/28;C22B4/00;C21C5/54;C21B3/00;

  • 国家 IN

  • 入库时间 2022-08-21 12:51:26

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号