首页> 外国专利> A PROCESS FOR THE PRODUCTION OF GEOPOLYMER CEMENT FROM FLY ASH AND GRANULATED BLAST FURNACE SLAG, COPOLYMER CEMENT MADE THEREBY AND PROCESS OF MAKING PRODUCTS THEREOF

A PROCESS FOR THE PRODUCTION OF GEOPOLYMER CEMENT FROM FLY ASH AND GRANULATED BLAST FURNACE SLAG, COPOLYMER CEMENT MADE THEREBY AND PROCESS OF MAKING PRODUCTS THEREOF

机译:用粉煤灰和粒状高炉矿渣生产地聚物水泥的方法,由此制成的共聚物水泥及其制造方法

摘要

The process for the production of geopolymer cement from fly ash and granulated blast furnace slag uses very high proportion (60 to 95%) of industrial waste such as fly ash and granulated blast furnace slag. In the process granulated blast furnace slag is fine grounded and/or mechanically activated in conventional grinding mills or high-energy mills. The fly ash, which is found in powder form and fine powder of granulated blast furnace slag, is thoroughly mixed with sodium or potassium based alkaline activator and water. The paste is cured at room temperature during which the dissolution of silica and alumina present if fly ash and granulated blast furnace slag starts. After the initial dissolution, the paste is heat treated at the temperature in the range of 60-200 degree C. The process does not require large energy consumption and also produces no CO2 emission. Also the processing steps are simple and easy.[IN-DEL-2006-00728A]
机译:由粉煤灰和粒状高炉矿渣生产地聚合物水泥的过程使用了很高比例(60%至95%)的工业废物,例如粉煤灰和粒状高炉矿渣。在此过程中,颗粒状的高炉矿渣在常规磨机或高能磨机中被细磨和/或机械活化。粉煤灰以粉末状和高炉矿渣的细粉形式存在,并与钠或钾基碱性活化剂和水充分混合。糊状物在室温下固化,在此期间,如果开始产生粉煤灰和高炉矿渣,则会溶解二氧化硅和氧化铝。初始溶解后,将糊状物在60-200摄氏度的温度范围内进行热处理。该过程不需要大量的能耗,也不会产生CO2排放。而且,处理步骤也很简单。[IN-DEL-2006-00728A]

著录项

  • 公开/公告号IN291555B

    专利类型

  • 公开/公告日2018-01-12

    原文格式PDF

  • 申请/专利权人

    申请/专利号IN728/DEL/2006

  • 发明设计人

    申请日2006-03-20

  • 分类号

  • 国家 IN

  • 入库时间 2022-08-21 12:51:35