The invention relates to a process for producing low alloy steel comprising the steps of: casting a steel alloy with composition 0.10 to 0.25 - carbon, 1.0 – 1.8 Manganese, 0.40 – 0.6 Silicon, 0.15 – 0.25 Chromium, 0.10 – 0.15 Molybdenum, 0.40 – 0.65 Nickel, 0.34 – 0.69 Carbon equivalent, 0 – 0.01 Vanadium, 0 -0.08 Titanium, 0 – 0.01 Boron, balance being Iron and residual impurities (in wt.%); homogenizing the steel alloy by austenitizing at 1150-1200°C for 30-45 minutes; and direct by water quenching to room temperature.
机译:本发明涉及一种生产低合金钢的方法,该方法包括以下步骤:铸造具有以下成分的钢合金:碳0.10至0.25-碳,1.0-1.8锰,0.40-0.6硅,0.15-0.25铬,0.10-0.15钼,0.40- 0.65镍,0.34 – 0.69碳当量,0 – 0.01钒,0 -0.08钛,0 – 0.01硼,余量为铁和残留杂质(以重量%计);通过在1150-1200℃下奥氏体化30-45分钟来使钢合金均质化;然后直接用水淬火至室温。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号