Provided are a method for deriving a cooling time when quenching a steel material, a method for quenching a steel material and a method for quenching and tempering a steel material. The method for deriving a cooling time comprises: step A of cooling a test specimen heated to a cooling initiation temperature Ts under a cooling condition C and measuring the cooling time t until the temperature of a center portion of the test specimen reaches a cooling termination temperature Te; step B of determining a function f which is defined by t = f(V/S) and which is satisfied by data including the volume V, the surface area S and the cooling time t of the test specimen obtained in step A; and step C of substituting the volume V1 and the surface area S1 of the shape F1 of a steel material to be actually quenched in the relational expression t = f(V/S), and calculating a cooling time t1. The method for quenching a steel material comprises: actually heating the steel material to be quenched to the cooling initiation temperature Ts; cooling only for the cooling time t1 under the cooling condition C; and then stopping cooling under the cooling condition C. The method for quenching and tempering a steel material comprises tempering the steel material quenched by this method.
展开▼