Combination of support material and model material and support material applied to three-dimensional modeling method using ink jet stereolithography apparatus

机译:支撑材料和模型材料的组合以及使用喷墨立体光刻设备应用于三维建模方法的支撑材料

摘要

PROBLEM TO BE SOLVED: To provide a model material applied to a three-dimensional molding method by an inkjet optical molding method extremely low in swelling due to water or moisture absorption, or moisture absorption deformation during optical curing and after curing.SOLUTION: A model material contains a monofunctional ethylenic unsaturated monomer (A) having weighted average of SP value of 10 or less, a polyfunctional ethylenic unsaturated monomer (B) containing no urethane group having weighted average of SP value of 10 or less and an urethane-containing ethylenic unsaturated monomer (C) having weighted average of SP value of 10.9 or less, further contains a photoinitiator (D) with the content of (B) of 3 to 25%, the content of (C) of 5 to 35%, the content of (D) of 0.1 to 10% based on weight of the model material and weighted average of SP values of the curable resin component (A) to (C) of the model material of 9.0 to 10.3.SELECTED DRAWING: Figure 1
机译:要解决的问题:提供一种通过喷墨光学成型方法应用于三维成型方法的模型材料,该方法由于吸水或吸湿或在光学固化期间以及固化后吸湿变形而导致的溶胀极低。该材料包含SP值的平均值为10以下的单官能烯键式不饱和单体(A),SP值的平均值为10以下的不包含氨基甲酸酯基的多官能烯键式不饱和单体(B)和含氨基甲酸酯的烯键式不饱和键重均SP值为10.9或更小的单体(C),进一步包含光引发剂(D),其(B)的含量为3至25%,(C)的含量为5至35%, (D)为模型材料重量的0.1%到10%,以及可固化树脂组分的SP值的加权平均值为9.0%到10.3%的模型材料的(A)至(C)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号