FIELD: chemistry; electricity.;SUBSTANCE: invention relates to electroplating. Method for regeneration of chromium plating electrolyte Cr(III) using device for regeneration, containing electrolyte regeneration and cooling baths, involves heating of electrolyte, extracted from main chromium plating bath, to higher temperature than that at which chromium plating is conducted, and cooling of heated electrolyte to temperature is equal to or higher than that at which chromium plating is conducted, and lower than temperature of heating, and return of electrolyte to main bath. Method of chromium plating Cr(III) is performed using chromium plating installation including major and minor baths and Cr(III) electrolyte regeneration device, wherein method involves passing electric current between substrate-cathode and anode in main bath containing ions of Cr(III) and reducing agent, and electrolyte regeneration specified above.;EFFECT: reduced concentration of Cr(VI) ions formed during plating.;8 cl, 4 tbl, 1 dwg
机译:领域:化学;物质:本发明涉及电镀。使用包含电解质再生和冷却浴的再生装置再生铬电镀电解质Cr(III)的方法涉及将从主铬电镀浴中提取的电解质加热到比进行铬电镀时更高的温度,并冷却加热后的电解液的温度等于或高于进行镀铬的温度,并且低于加热温度,并使电解液返回主槽。镀铬的方法Cr(III)使用包括主槽和副槽以及Cr(III)电解液再生装置的镀铬设备进行,其中该方法涉及在包含Cr(III)离子的主槽中的衬底阴极和阳极之间通过电流效果:降低电镀过程中形成的Cr(VI)离子的浓度; 8 cl,4 tbl,1 dwg

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号