Provide a kind of manufacture nanometer hybrid organic-inorganic film, the organic-inorganic hybrid film that nanoporous is manufactured by same procedure, the application of nanoporous color separation film. More specifically, the present invention provides a kind of manufacture nanometer hybrid organic-inorganic film, include the following steps: that preparing organosol contains the compound with amino, there is isocyanate group and solvent; Mixed liquor is produced by increasing inorganic oxide precursor to organosol; With form organic molecular network, wherein described organic and inorganic molecule makes achievement peptization glue be a kind of reticular structure, positioned at the organic molecule reticular structure along the surface by heat treatment mixed solution. Method of the invention can be easily manufactured nano-pore hybrid organic-inorganic film and simply use the pectization organosol and condensation reaction inorganic oxide precursor by manufacturing process with three-dimensional microstructure. In addition, nanoporous color separation film is had using the organic-inorganic hybrid film of the nanoporous, big specific surface area can be provided with high-transmission rate and high solute removes efficiency. ;The 2016 of copyright KIPO submissions
机译:提供一种制造纳米杂化有机-无机薄膜的方法,纳米多孔的有机-无机杂化膜是通过相同的步骤制造的,纳米多孔分色膜的应用。更具体地说,本发明提供了一种制备纳米杂化有机-无机薄膜的方法,其包括以下步骤:制备有机溶胶中含有具有氨基的化合物,存在异氰酸酯基和溶剂;混合液是通过将无机氧化物前体增加到有机溶胶中而制得的;利用形成的有机分子网络,其中所述的有机和无机分子使成胶胶成为一种网状结构,通过热处理混合溶液沿表面位于有机分子网状结构处。本发明的方法可以容易地制造纳米孔杂化的有机-无机薄膜,并且可以通过具有三维微观结构的制造工艺简单地使用果胶化有机溶胶和缩合反应无机氧化物前体。另外,通过使用纳米多孔质的有机-无机杂化膜来形成纳米多孔质的分色膜,可以提供比表面积大,透射率高,溶质去除效率高的特征。 ; 2016年版权KIPO提交文件

著录项

  • 公开/公告号KR20160007756A

    专利类型

  • 公开/公告日2016-01-21

    原文格式PDF

  • 申请/专利权人 GWANGJU INSTITUTE OF SCIENCE AND TECHNOLOGY;

    申请/专利号KR20140079528

  • 发明设计人 JEON EUN KYUNG;PARK JI WOONG;

    申请日2014-06-27

  • 分类号C08J5/18;C08G18/83;C08G77/458;C08G79/00;C08K3/10;

  • 国家 KR

  • 入库时间 2022-08-21 14:15:15

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号