MANUFACTURE OF NEAR-NET SHAPE TITANIUM ALLOY ARTICLES FROM METAL POWDERS BY SINTERING WITH ATOMIC HYDROGEN

机译:金属粉末烧结制备金属粉末近净形钛合金制品

摘要

Disclosed is a process of forming a near-net shaped article that includes: (a) forming a powder blend by mixing commercially pure titanium powder and one or more hydrogenated titanium powders; (b) consolidating the powder blend to provide a green compact; c) heating the green compact to around 100 degrees to 250 degrees C; (d) forming beta-phase titanium and releasing atomic hydrogen by heating the green compact to around 400 to 600 degrees C; (e) reducing surface oxides on the titanium powder by heating the green compact to around 600 to 700 degrees C; (f) diffusion-controlled chemical homogenizing and densification of the green compact by heating the green compact to around 800 to 850 degrees C; (g) heating the cleaned and refined green compact in vacuum to around 1000 to 1350 degrees C to form a sintered dense compact; (h) cooling the sintered dense compact to form a near-net shaped article
机译:公开了一种形成近净形制品的方法,该方法包括:(a)通过混合市售纯钛粉末和一种或多种氢化钛粉末形成粉末共混物; (b)固结粉末混合物以提供生坯; c)将生压坯加热至约100℃至250℃; (d)通过将生坯加热至约400至600℃,形成β相钛并释放原子氢; (e)通过将生坯加热至约600至700℃来减少钛粉末上的表面氧化物; (f)通过将生坯加热到约800至850℃来控制生坯的扩散控制化学均质化和致密化; (g)将经清洁和精制的生坯在真空中加热至约1000至1350摄氏度,以形成烧结的致密坯; (h)冷却烧结的致密坯料以形成近净形制品

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号