The present invention relates to a process to prepare a salt product containing sodium chloride (NaCl) and at least one additive, wherein the salt product has a particle size of from 50 m to 10 mm, which process comprises the steps of: a) optionally, crushing a sodium chloride-containing material to a particle size that is between 1,000 times smaller and 3 times smaller than the size of the final salt product; b) optionally, crushing the at least one additive starting material to a particle size that is between 0.5 and 2 times the particle size of the sodium chloride-containing material particles resulting from step a.); c) subsequently, mixing the sodium chloride-containing material particles of a particle size that is between 1,000 times smaller and 3 times smaller than the size of the final salt product, and additive particles of a particle size that is between 0.5 and 2.0 times the particle size of the sodium chloride-containing material particles; d) subsequently, compacting the particle mixture resulting from step c.) using a pressure of from 40 to 400 MPa; e. subsequently, crushing the compacted salt product to give particles of the desired particle size of 50 m to 10 mm; wherein the steps are carried out under substantially dry conditions. Additionally, the invention provides the low sodium salt product obtainable by the process and the use thereof for human or animal consumption.
机译:本发明涉及一种制备包含氯化钠(NaCl)和至少一种添加剂的盐产品的方法,其中该盐产品的粒度为50m-10mm,该方法包括以下步骤:a)任选地,将含氯化钠的物料压碎成比最终盐产品的粒径小1,000倍至3倍的粒径; b)任选地,将至少一种添加剂原料压碎至粒度为步骤a。)所得的含氯化钠的材料颗粒的粒度的0.5至2倍; c)随后,将粒径小于最终盐产物粒径1,000倍至3倍的含氯化钠材料颗粒与粒径为最终盐产物的0.5至2.0倍的添加剂颗粒混合。含氯化钠的材料颗粒的粒径; d)随后,使用40至400MPa的压力将由步骤c。)得到的颗粒混合物压实; e。随后,将压实的盐产物压碎,得到所需粒度为50m至10mm的颗粒;其中所述步骤在基本上干燥的条件下进行。另外,本发明提供了可通过该方法获得的低钠盐产品及其在人类或动物消费中的用途。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号