FIELD: metallurgy.;SUBSTANCE: invention relates to metallurgy of ferrotitanium production, containing 28-40 wt % of titanium, which is in demand in industry for production of welding electrodes, for alloying of structural, stainless, fireproof steels. To produce ferrotitanium by double-stage aluminothermal method, a charge is developed with the following composition, wt %: ilmenite concentrate with content of TiO2 52-54 wt % 26.6-27.8, secondary aluminium 21.0-27.0, lime with carbon content of not more than 0.3 wt % 4.5-4.9, iron scale 13.2-14.4, ferrosilicon 75% 0.3-0.9, steel scrap 0.5-3.4, ground titanium-containing slag 26.6-29.0, at the same time the titanium-containing slag as a component of the titanium-containing charge is produced in an electric furnace by melting of the charge containing, wt %: ilmenite concentrate with content of TiO2 63-65 wt % 75.5-79.2, secondary aluminium 4.9-5.8, lime with carbon content of not more than 0.6 wt % 12.0-13.2, iron scale 2.6-3.8, ferrosilicon 75% 2.6-2.8, after soaking of the melt they drain metal and titanium-containing slag, which is separated, cooled and ground.;EFFECT: invention makes it possible to use new titanium-containing charge compositions without rutile concentrate.;3 cl, 3 tbl
机译:钛合金的生产冶金技术领域本发明涉及含有28-40wt%的钛的钛铁合金的生产冶金,工业上用于生产用于结构钢,不锈钢,耐火钢的合金的焊接电极。为了通过两阶段铝热法生产铁钛合金,需制造具有以下重量百分比组成的装料:wt%的钛铁矿精矿,其中TiO 2 的含量为26.6-27.8 wt%,次生铝为21.0-27.0 ,碳含量不超过0.3重量%的石灰4.5-4.9,铁鳞13.2-14.4,硅铁75%0.3-0.9,废钢0.5-3.4,磨碎的含钛渣26.6-29.0,同时钛在电炉中,通过熔化含有TiO 2 含量为63-65 wt%75.5-79.2的wt%钛铁矿精矿的装料,在电炉中生产含钛渣,二次铝4.9-5.8,含碳量不超过0.6重量%的12.0-13.2石灰,铁垢2.6-3.8,硅铁75%2.6-2.8,在熔体浸泡后,它们会排出金属和含钛炉渣,分离;冷却并研磨。;效果:本发明可以使用不含金红石的新型含钛进料组合物精矿; 3 cl,3 tbl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号