Provided is a molten salt bath which is used to dissolve a WC-Co super-hard alloy and which is obtained by homogeneously melting a molten alkali nitrate in a molten alkali chloride, wherein at least two compounds selected from among the group consisting of MCl (M = Li, Na or K) are selected as the alkali chloride and at least one compound selected from among the group consisting of NNO3 (N = Li, Na or K) is selected as the alkali nitrate. The at least two alkali chloride compounds selected from among the group consisting of MCl (M = Li, Na or K) are contained at a concentration of 1 mol.% or higher, and preferably 1-20 mol.%, and the alkali nitrate is contained at a concentration of 99-80 mol.%. This molten salt bath dissolves a WC-Co super-hard alloy at a low temperature, reduces corrosion damage to a reactor plant vessel used to dissolve a WC-Co super-hard alloy, and enables industrial scale recovery of tungsten and cobalt.
机译:提供一种熔融盐浴,其用于溶解WC-Co超硬合金,并且是通过将熔融硝酸盐在熔融碱金属氯化物中均匀地熔融而获得的,其中至少两种化合物选自由MCl(选择M = Li,Na或K作为碱金属氯化物,并且选自NNO 3 中的至少一种化合物(N = Li,Na或K)作为碱金属硝酸盐。 。选自由MCl(M = Li,Na或K)组成的组中的至少两种碱金属氯化物,其浓度为1mol。%或更高,优选为1-20mol。%,以及所述碱金属硝酸盐。所含浓度为99-80摩尔%。该熔融盐浴在低温下溶解WC-Co超硬合金,减少了对用于溶解WC-Co超硬合金的反应堆工厂容器的腐蚀损害,并能够工业规模回收钨和钴。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号