首页> 外国专利> Production method of the heatproof magnesium alloy and its heatproof magnesium alloy which are superior in fatigue at elevated temperature strength quality and heatproof part null mass

Production method of the heatproof magnesium alloy and its heatproof magnesium alloy which are superior in fatigue at elevated temperature strength quality and heatproof part null mass

机译:高温疲劳强度优异且耐热零件零质量的耐热镁合金及其耐热镁合金的制造方法

摘要

PROBLEM TO BE SOLVED: To provide a heat-resistant magnesium alloy excellent in high temperature fatigue strength characteristics, a method of manufacturing the heat-resistant magnesium alloy and heat-resistant parts for an engine manufactured by using the heat-resistant magnesium alloy.;SOLUTION: The magnesium alloy includes, in mass%, Y of 1.8 to 8% and Sm and/or Nd of 1.4 to 8% in total amounts with the remainder consisting of Mg and inevitable impurities. The mean crystal grain size of the crystal grains of a magnesium alloy structure falls within the range of 10 to 50 μm, and 10 or more pieces of plate-like precipitates each having a major axis of 5 μm or more and an aspect ratio of 10 or more are precipitated in the crystal grains. Further, preferably, Ho of 0.5 to 2% is contained.;COPYRIGHT: (C)2012,JPO&INPIT
机译:解决的问题:为了提供一种具有优异的高温疲劳强度特性的耐热镁合金,提供了一种制造耐热镁合金的方法以及使用该耐热镁合金制造的用于发动机的耐热部件的方法。溶液:镁合金的质量百分比为Y,总量为1.8%至8%,Sm和/或Nd总量为1.4%至8%,其余部分由Mg和不可避免的杂质组成。镁合金结构的晶粒的平均晶粒尺寸在10〜50μm的范围内,长轴为5μm以上且长径比为10的10个以上的板状析出物。或更多的沉淀在晶粒中。另外,优选含有0.5〜2%的Ho。版权所有:(C)2012,JPO&INPIT

著录项

  • 公开/公告号JP5530317B2

    专利类型

  • 公开/公告日2014-06-25

    原文格式PDF

  • 申请/专利权人 株式会社神戸製鋼所;

    申请/专利号JP20100202897

  • 发明设计人 有賀 康博;長尾 護;難波 茂信;

    申请日2010-09-10

  • 分类号C22C23/06;C22F1/06;C22F1/00;

  • 国家 JP

  • 入库时间 2022-08-21 16:15:14