首页> 外国专利> MANUFACTURING METHOD OF LITHIUM TARGET FOR MEDICAL ACCELERATOR-DRIVEN COMPACT NEUTRON SOURCE

MANUFACTURING METHOD OF LITHIUM TARGET FOR MEDICAL ACCELERATOR-DRIVEN COMPACT NEUTRON SOURCE

机译:医用致动器驱动的紧凑中子源锂靶的制备方法

摘要

PROBLEM TO BE SOLVED: To manufacture a large-sized lithium target in which, for example, the diameter×thickness of a conjugate of an Li membrane/Cu cooling base is settled within the range of φ20 mm to 40 mm×100 to 200 μm±10 μm.;SOLUTION: A manufacturing method of a lithium target includes the steps of: placing, on a hot plate, a Cu cooling base constituting the lithium target; heating the Cu cooling base in a nitrogen containing atmosphere by means of the hot plate with the precision of 20 to 70°C±0.1°C; placing an Li membrane on the Cu cooling base while heating the Cu cooling base by means of the hot plate, and temporarily bonding both the Li membrane and the Cu cooling base by pressing them using a roller; and then detaching a conjugate of the Li membrane/Cu cooling base from the hot plate and joining both the Li membrane and the Cu cooling base within several seconds under the condition that the pressure is 15 to 25 MPa and the temperature is within the range of 20 to 70°C±0.1°C.;COPYRIGHT: (C)2014,JPO&INPIT
机译:解决的问题:为了制造大型锂靶,例如,将Li膜/ Cu冷却基体的共轭物的直径×厚度固定在φ20mm至40mm×100至200μm的范围内±10μm;解决方案:锂靶的制造方法包括以下步骤:在加热板上放置构成锂靶的Cu冷却基体;借助于热板在含氮气氛中加热Cu冷却基,精度为20〜70℃±0.1℃。在通过热板加热Cu冷却基座的同时,将Li膜放置在Cu冷却基座上,并通过用辊压将Li膜和Cu冷却基座两者临时结合;然后在15至25 MPa的压力和温度范围内的条件下,在几秒钟内从热板上取下Li膜/ Cu冷却基体的共轭物,并连接Li膜和Cu冷却基体。 20至70°C±0.1°C .;版权所有(C)2014,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号