首页> 外国专利> Method for heat treatment of casting component made of aluminum silicon alloy, used in travel carriage of motor vehicle, involves quenching components of solution and annealing solution at specific temperature for predetermined time

Method for heat treatment of casting component made of aluminum silicon alloy, used in travel carriage of motor vehicle, involves quenching components of solution and annealing solution at specific temperature for predetermined time

机译:用于机动车辆的旅行车厢的由铝硅合金制成的铸造部件的热处理方法,包括在特定温度下将溶液和退火溶液的部件淬火预定时间。

摘要

The method involves quenching and storing components of a solution. The annealing of the solution is performed (14) at a temperature of 460-530[deg] C for time duration 2-30 minutes. The external storage of the solution is performed (16) at a temperature of 230-320[deg] C for time duration of 2-65 minutes. An independent claim is included for casting component.
机译:该方法涉及淬灭和储存溶液的组分。溶液的退火在460-530℃的温度下进行(14)持续2-30分钟的时间。溶液的外部储存在230-320℃的温度下进行(16)持续2-65分钟的时间。铸造零件包括独立索赔。

著录项

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号