PURPOSE: a kind of nano silver/silicon dioxide gel finishing solution that makes is provided for being decreased or increased particle size or bonds nano silver particles in the silica solution of hydro-thermal process and control granular size and shape;CONSTITUTION: the step of manufacturing method of a kind of nanometer of silver/silicon dioxide includes: that sol coating(method) solution is put into one or more compounds and is selected from NaOH, and KOH, NH4OH are added active silica aqueous solution and simultaneously stabilize active silicate; Step: the solution of reproducibility is manufactured by by a kind of reducing agent to stable active silicic acid solution; It reduces silver-colored step and reducing solution is added by injecting silver-colored precursor solution; With the mixture reduction step after hydro-thermal process. Silver-colored precursor A gNO3 or AgCl. ;The 2013 of copyright KIPO submissions;[Reference numerals] (AA) step manufactures active silicic acid; (BB) step stablizes active silicic acid; (CC) solution of step manufacture reproducibility; (DD) step reduces silver; (EE) the hydro-thermal treatment of step
机译:用途:一种纳米银/二氧化硅凝胶整理液,用于减小或增加粒径或在水热法二氧化硅溶液中键合纳米银粒子,并控制粒度和形状;组成:以下步骤一种纳米级银/二氧化硅的制备方法,包括:将溶胶涂层法置于一种或多种化合物中,并从NaOH中选择,并在KOH,NH4OH中加入活性二氧化硅水溶液,同时稳定活性硅酸盐。步骤:用一种还原剂还原成稳定的活性硅酸溶液,制成溶液的重现性。它减少了银色的步骤,并通过注入银色的前体溶液添加了还原溶液;经过水热处理后的混合物还原步骤。银色前体A gNO3或AgCl。 ; 2013年版权KIPO提交文件; [参考数字](AA)步骤生产活性硅酸; (BB)步骤稳定活性硅酸; (CC)分步制造可重复性的解决方案; (DD)步骤减少了白银; (EE)水热处理步骤

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号