, where n, k and m denote the number of radicals per molecule, where n equals an integer from 1 to 5; k equals an integer from 0 to 4; m equals an integer from 0 to 10. The method of producing compounds of formula (1) involves adding a sodium hydride solution to fluorinated alcohol with defined number n, k and m in a current of argon and ethylene chlorohydrin. The mixture is heated on an oil bath under a vacuum. The fraction of oxyalkylated fluorinated alcohol is distilled, to which water and potassium hydroxide is then added. After dissolution of potassium hydroxide, carbon disulphide is added at temperature not higher than 30°C. The end product is extracted. A method for floatation benefication of sulphide ore is also disclosed. The method involves crushing sulphide ore in an aqueous medium to form pulp. The pulp is conditioned with a foaming agent and a compound of formula (1), taken in amount of 25-150 g per ton of crushed material. Floatation is carried out with extraction of sulphides into the foamed product.;EFFECT: more complete utilisation of sulphide ore owing to higher intensity of the floatation process while using fluorinated potassium xanthogenates, higher intensity of the floatation process for copper and nickel minerals when processing Cu-Ni ore.;4 cl, 7 dwg, 4 tbl, 2 ex"/> FLUORINATED POTASSIUM XANTHOGENATES, SYNTHESIS METHODS THEREOF AND USE IN FLOTATION BENEFICATION OF SULPHIDE ORE
首页> 外国专利> FLUORINATED POTASSIUM XANTHOGENATES, SYNTHESIS METHODS THEREOF AND USE IN FLOTATION BENEFICATION OF SULPHIDE ORE

FLUORINATED POTASSIUM XANTHOGENATES, SYNTHESIS METHODS THEREOF AND USE IN FLOTATION BENEFICATION OF SULPHIDE ORE

机译:氟化黄原酸钾,合成方法及其在硫化矿浮选中的应用

摘要

FIELD: chemistry.;SUBSTANCE: invention relates to novel compounds for floatation benefication of polymetallic and other types of sulphide ore and synthesis method thereof used in mining industry. Compounds which are fluorinated potassium xanthogenates are described by formula (1): , where n, k and m denote the number of radicals per molecule, where n equals an integer from 1 to 5; k equals an integer from 0 to 4; m equals an integer from 0 to 10. The method of producing compounds of formula (1) involves adding a sodium hydride solution to fluorinated alcohol with defined number n, k and m in a current of argon and ethylene chlorohydrin. The mixture is heated on an oil bath under a vacuum. The fraction of oxyalkylated fluorinated alcohol is distilled, to which water and potassium hydroxide is then added. After dissolution of potassium hydroxide, carbon disulphide is added at temperature not higher than 30°C. The end product is extracted. A method for floatation benefication of sulphide ore is also disclosed. The method involves crushing sulphide ore in an aqueous medium to form pulp. The pulp is conditioned with a foaming agent and a compound of formula (1), taken in amount of 25-150 g per ton of crushed material. Floatation is carried out with extraction of sulphides into the foamed product.;EFFECT: more complete utilisation of sulphide ore owing to higher intensity of the floatation process while using fluorinated potassium xanthogenates, higher intensity of the floatation process for copper and nickel minerals when processing Cu-Ni ore.;4 cl, 7 dwg, 4 tbl, 2 ex
机译:技术领域本发明涉及用于多金属和其他类型的硫化矿的浮选精矿的新型化合物及其在采矿业中使用的合成方法。氟化黄原酸钾的化合物由式(1)描述:,其中n,k m表示每个分子的基团数,其中n等于1至5的整数; k等于0到4的整数; m等于0至10的整数。制备式(1)的化合物的方法包括在氩气和乙烯氯醇的气流中将氢化钠溶液加入到定义为n,k和m的氟化醇中。将混合物在真空下的油浴上加热。蒸馏馏分氧烷基化的氟化醇,然后向其中加入水和氢氧化钾。氢氧化钾溶解后,在不高于30℃的温度下加入二硫化碳。提取最终产品。还公开了一种用于硫化矿浮选的方法。该方法包括在水性介质中将硫化矿石破碎以形成纸浆。纸浆用发泡剂和式(1)的化合物调理,其用量为每吨压碎材料25-150 g。浮选是通过将硫化物提取到泡沫产品中来进行的;效果:由于使用氟化钾黄原酸钾时浮选过程的强度更高,硫化铜矿石的利用率更高,加工铜和镍矿物时浮选过程的强度更高-镍矿; 4 cl,7 dwg,4 tbl,2 ex