INNER LINER RUBBER COMPOSITION IMPROVING ANTI-AIR PERMEABILITY BY INCLUDING LIQUID PHASE POLYBUTENE, AND A TIRE COMPRISING RUBBER WITH EXCELLENT ANTI-AIR PERMEABILITY AND PHYSICAL PROPERTIES AS AN INNER LINER

机译:内衬橡胶组合物,包括液相聚丁烯,可改善抗空气渗透性;轮胎内衬具有优异的抗空气渗透性和物理性能,可构成轮胎

摘要

PURPOSE: An inner liner rubber composition is provided to improve an anti-air permeability by liquid phase polybutene, and to improve physical properties because of improved dispersibility of reinforcing filler by a dispersion aid.;CONSTITUTION: An inner liner rubber composition comprises 10-20 parts by weight of liquid polybutene, on the basis of 100.0 parts by weight of raw rubber. The raw rubber consists of 20-40 parts by weight of natural rubber, and 60-80 parts by weight of halobutyl rubber. A tire comprises rubber consisting of the rubber composition as an inner liner. The liquid polybutene has weight average molecular weight of 1,200-1,400, the viscosity at 40 °C is 20,000-25,000 cP, and the viscosity at 100 °C is 550-750 cP.;COPYRIGHT KIPO 2012
机译:用途:提供内衬橡胶组合物以改善液相聚丁烯的抗空气渗透性,并由于分散剂对增强填料的分散性改善而改善物理性能。;组成:内衬橡胶组合物包含10-20以100.0重量份生橡胶为基础,液体聚丁烯重量份。生橡胶由20-40重量份的天然橡胶和60-80重量份的卤化丁基橡胶组成。轮胎包括由橡胶组合物组成的橡胶作为内衬层。液体聚丁烯的重均分子量为1,200-1,400,在40℃下的粘度为20,000-25,000 cP,在100℃下的粘度为550-750 cP。; COPYRIGHT KIPO 2012

著录项

  • 公开/公告号KR20120038235A

    专利类型

  • 公开/公告日2012-04-23

    原文格式PDF

  • 申请/专利权人 KUMHO TIRE CO. INC.;

    申请/专利号KR20100099877

  • 发明设计人 BEAK HOON SUN;

    申请日2010-10-13

  • 分类号C08L23/22;C08L23/28;C08L7/00;B60C5/14;

  • 国家 KR

  • 入库时间 2022-08-21 17:10:11