The present invention relates to a semi-rigid road paving method and a composition for cement milk used in the method and a construction method for injecting the same. The semi-rigid road paving method according to the present invention includes the steps of laying and compacting asphalt, and injecting cement milk into the voids in the asphalt, applying vibration to the cement milk, and cement milk into the voids in the asphalt. It is characterized by promoting the injection. The injection material composition for cement milk used in the present invention is 50 to 90% by weight of flame resistant cement, 3 to 30% by weight of fastener, 0.1 to 5% by weight of a fluidizing agent, 0.01 to 1.0% by weight of thickener, and 1 to 15% by weight of silica fume. %, 1 to 12% by weight of the expansion material, 0.1 to 2% by weight of the hydration accelerator and 0.1 to 3% by weight of the hydration delay agent.
机译:半刚性铺路方法以及用于该方法的用于水泥乳的组合物及其注入方法技术领域本发明涉及一种半刚性铺路方法以及用于该方法的用于水泥乳的组合物及其注入方法。根据本发明的半刚性铺路方法包括以下步骤:铺设并压实沥青,将水泥乳注入到沥青中的空隙中,对水泥乳施加振动,并且将水泥乳注入到沥青中的空隙中。它的特点是促进注射。用于本发明的用于水泥乳的注射材料组合物是50至90重量%的耐火水泥,3至30重量%的紧固件,0.1至5重量%的流化剂,0.01至1.0重量%。增稠剂,和1至15重量%的硅粉。 1%,1%至12%重量的膨胀材料,0.1%至2%重量的水合促进剂和0.1%至3%重量的水合延迟剂。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号