摘要

PURPOSE: A method for dyeing fabric containing multi-layered conductive yarn covered with nylon and cotton fiber is provided to ensure excellent color fastness and shape stability. CONSTITUTION: A method for dyeing conductive fabric containing multi-layered conductive yarn comprises: a step of mixing 8-10 g/L of hydrogen peroxide, 3-5 g/L of stabilizing agent, 2-4 g/L of refining agent, 1-3 g/L of NaOH, and remaining amount of water to prepare a refining/bleaching agent; a step of refining/bleaching using the refining/bleaching agent at 80-85C for 30-40 minutes and drying at room temperature; a step of preparing dyeing solution containing 2-13% of o.w.f, 40-60 g/L of Na_2SO_4, 15-20 g/L of Na_2CO_3, and remaining amount of water and dyeing at 40-80C for 60-90 minutes; and a step of soaping at 60-70C for 20-30 minutes.
机译:目的:提供一种染色织物的方法,该织物包含被尼龙和棉纤维覆盖的多层导电纱,以确保优异的色牢度和形状稳定性。组成:一种用于染色包含多层导电纱的导电织物的方法,该方法包括以下步骤:将8-10 g / L的过氧化氢,3-5 g / L的稳定剂,2-4 g / L的精制剂混合, 1-3 g / L NaOH和剩余量的水以制备精制/漂白剂;使用精制/漂白剂在80-85℃下精制/漂白30-40分钟并在室温下干燥的步骤;制备染色溶液的步骤,该溶液包含2-13%的质量分数,40-60g / L的Na_2SO_4、15-20g / L的Na_2CO_3和剩余量的水,并在40-80℃下染色60-90分钟;然后在60-70℃皂洗20-30分钟。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号