首页> 外国专利> MODIFICATION ADDITIVE FOR ASPHALT MASSES AND TYPE AND MANNER OF ASPHALT PRODUCTION FOR THE CREATION OF MINERAL-ASPHALT MIXTURES HAVING A HIGH SHEAR MODULUS

MODIFICATION ADDITIVE FOR ASPHALT MASSES AND TYPE AND MANNER OF ASPHALT PRODUCTION FOR THE CREATION OF MINERAL-ASPHALT MIXTURES HAVING A HIGH SHEAR MODULUS

机译:沥青质的改性助剂以及制备高剪切模量的矿物-沥青混合物的沥青生产类型和方式

摘要

The invention relates to a modification additive for asphalt masses and to the manner of production of asphalt masses for the creation of mineral-asphalt mixtures having a high shear modulus. The essence of the invention is a modifier, characterized in that it comprises 50 to 97% of cyclopentadiene oligomers, which are dissolved in 2 to 30% by weight of alkenes with 9-11 carbon atoms in a molecule, and 1 to 15% by weight of cyclic and aromatic olefins, wherein the latter are segregation residues of other hydrocarbon fractions. The liquid asphalt mass is added to the above-mentioned modifier in a quantity of 0.1 to 15% by weight at a temperature of no more than 185ºC and kept in a liquid state for at least 15 minutes. The modified asphalt obtained in this way, together with the mineral additive, forms mineral-asphalt mixtures having a high shear modulus.
机译:本发明涉及一种用于沥青料的改性添加剂,以及涉及用于产生具有高剪切模量的矿物-沥青混合物的沥青料的生产方式。本发明的本质是改性剂,其特征在于它包含50-97%的环戊二烯低聚物,其溶解在2-30重量%的分子中具有9-11个碳原子的烯烃中,和1-15重量%。环和芳烃的重量,其中后者是其他烃馏分的偏析残基。在不超过185℃的温度下,将液态沥青物料以0.1至15重量%的量添加到上述改性剂中,并保持液态至少15分钟。以这种方式获得的改性沥青与矿物添加剂一起形成具有高剪切模量的矿物沥青混合物。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号