PENETRATION ENHANCING FLUX FORMULATION FOR TUNGSTEN INERT GAS WELDING AUSTENITIC STAINLESS STEEL, METHOD OF WELDING USING SUCH FLUX AND WELDED ARTICLE FROM AUSLENITIC STAINLESS STEEL
PENETRATION ENHANCING FLUX FORMULATION FOR TUNGSTEN INERT GAS WELDING AUSTENITIC STAINLESS STEEL, METHOD OF WELDING USING SUCH FLUX AND WELDED ARTICLE FROM AUSLENITIC STAINLESS STEEL
展开▼
机译:钨惰性气体焊接奥氏体不锈钢的渗透增强焊剂配方,这种焊剂和奥氏体不锈钢焊接件的焊接方法
展开▼
页面导航
摘要
著录项
相似文献
摘要
A Penetration Enhancing Activating Flux (PEAF) in paste form for autogenous TIG welding of auslenitic stainless steels adapted for ready application with a brush on top weld surface prior to conducting autogenous TIG welding to favour single weld pass, of austenitic stainless steels of AISI304LN and AISI 316LN varieties with weld bead penetration up to a section thickness of 12 mm. Importantly, the above (PEAF) paste based TIG welding of the invention achieves increase in weld bead penetration of about 300 % over the conventional TIG process without activating flux. The PEAF paste based TIG welding also favours higher productivity and high quality apart from being cost-effective due to less requirement of consumables and controlled heat input to arrest distortion, making it widely acceptable for variety of industrial applications for welding of auslenitic stainless steel.
展开▼