首页> 外国专利> Method for leaching Copper sulfide ore with H2SO4 Solution comprising iodide ion and Ion Iron (iii) in excess of the iodide ion, reducing the concentration of iodine in the solution obtained after leaching, less than 1 mg / l to Charcoal and oxidize The Iron (ii) Ion using microbes oxidized Iron.

Method for leaching Copper sulfide ore with H2SO4 Solution comprising iodide ion and Ion Iron (iii) in excess of the iodide ion, reducing the concentration of iodine in the solution obtained after leaching, less than 1 mg / l to Charcoal and oxidize The Iron (ii) Ion using microbes oxidized Iron.

机译:用H2SO4溶液浸提硫化铜矿石的方法,该溶液含碘离子和离子铁(iii)过量的碘离子,将浸提后得到的溶液中的碘浓度降低至不足1 mg / l成为木炭并氧化铁(ii)使用微生物氧化的铁离子。

摘要

Method for leaching sulfide ore leaching of cu from cu comprising the Ore with H2SO4 Solution comprising iodide ion and Iron ion in excess of iodide ion.Reduce iodine leaching Solution obtained after less than 1 mg / l to Charcoal and oxidize The Iron (ii) Ion using microbes oxidize fe.
机译:一种从矿石中浸出含铜的硫化物矿石的方法,用含碘离子和铁离子(过量碘离子)的H2SO4溶液浸出铜,然后将少于1 mg / l的碘浸出溶液还原为木炭并氧化铁(ii)使用微生物的离子氧化铁。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号