PURPOSE: An early strength concrete composition including a high-early-strength admixture is provided to maintain a cure temperature of concrete without a heater, and to reduce the total construction time at the construction site.;CONSTITUTION: An early strength concrete composition contains water, aggregate, cement and high-early-strength admixture powder. The high-early-strength admixture contains 40~70wt% of calcium aluminate with the blaine surface area of 7,000~10,0000 square centimeters per gram, 15~30wt% of inorganic sulphate with the blaine surface area of 6,000~9,000 square centimeters per gram, 10~25wt% of calcium carbonate powder with the blaine surface area of 3,000~6,000 square centimeters per gram, and 0.1~10wt% of cellulosic fibers.;COPYRIGHT KIPO 2010
机译:目的:提供一种包括高早强掺合料的早强混凝土组合物,以在不使用加热器的情况下保持混凝土的固化温度,并减少施工现场的总施工时间。;组成:早强混凝土组合物含有水,骨料,水泥和高强度掺合料粉。高强度混合物含有40〜70wt%的铝酸钙,每平方米的blaine表面积为7,000〜10,0000平方厘米;含有15〜30wt%的无机硫酸盐,其blaine的表面积为每公斤6,000〜9,000平方厘米。克碳粉,碳酸钙粉的10〜25wt%,布兰比表面积为每克3,000〜6,000平方厘米和纤维素纤维的0.1〜10wt%。;COPYRIGHT KIPO 2010

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号