首页> 外国专利> The recovery process of copper smelting slag of copper and molybdenum includes the treatment of slag generated in copper thermal metallurgy production in the furnace, the maintenance of inert atmosphere in the furnace, the increase of slag temperature from 1200 to 1500 degrees, the maintenance of viscosity, quality transfer, grinding and processing.

The recovery process of copper smelting slag of copper and molybdenum includes the treatment of slag generated in copper thermal metallurgy production in the furnace, the maintenance of inert atmosphere in the furnace, the increase of slag temperature from 1200 to 1500 degrees, the maintenance of viscosity, quality transfer, grinding and processing.

机译:铜和钼的铜冶炼渣的回收过程包括:处理炉内铜热冶金生产中产生的炉渣,维持炉内惰性气氛,炉渣温度从1200度提高到1500度,维持粘度,质量转移,研磨和加工。

摘要

Recovery of copper and Molybdenum slag of Copper smelting slag Disposal includes Production pyrometallurgical Copper inside FurnaceMaintaining an Inert atmosphere in the Furnace, raise temperature of slag in 1200 and 1500 degrees, viscosity, Mass Transfer, and a grinding process.
机译:回收铜冶炼渣中的铜和钼渣处置包括在炉内生产火法冶金铜维持炉膛中的惰性气氛,将炉渣温度升高到1200和1500度,粘度,传质和研磨过程。

著录项

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号