摘要

Disclosed herein are a method of preparing Li-doped silica nanotubes using an anodic aluminum oxide (AAO) template, and a method of storing energy using the prepared Li-doped silica nanotubes. Unlike prior methods for preparing metal nanotubes, according to the disclosed preparation method, the Li-doped silica nanotubes having a uniform size can be easily obtained in mild conditions using a lithium precursor, a silica sol and an anodic aluminum oxide template. The preparation method comprises adsorbing the lithium precursor and the silica sol on the surface of the AAO template, drying the lithium precursor and the silica sol, adsorbed onto the AAO template, in a vacuum, to form nanotubes, and then drying the nanotubes. The Li-doped silica nanotubes prepared according to the disclosed method can be used as economical hydrogen storage materials, electrode materials for lithium secondary batteries, or energy storage sources for automobiles or other transportation means.
机译:本文公开了使用阳极氧化铝(AAO)模板制备掺锂的二氧化硅纳米管的方法,以及使用制备的掺锂的二氧化硅纳米管存储能量的方法。与用于制备金属纳米管的现有方法不同,根据所公开的制备方法,可以使用锂前体,硅溶胶和阳极氧化铝模板在温和条件下容易地获得具有均匀尺寸的掺Li的二氧化硅纳米管。制备方法包括将锂前体和硅溶胶吸附在AAO模板的表面上,将锂前体和硅溶胶在真空中干燥,吸附到AAO模板上以形成纳米管,然后干燥纳米管。根据所公开的方法制备的掺Li的二氧化硅纳米管可以用作经济的储氢材料,锂二次电池的电极材料或汽车或其他运输工具的储能源。

著录项

  • 公开/公告号US2010069236A1

    专利类型

  • 公开/公告日2010-03-18

    原文格式PDF

  • 申请/专利权人 HAE JIN KIM;

    申请/专利号US20070312227

  • 发明设计人 HAE JIN KIM;

    申请日2007-10-11

  • 分类号B01J20/04;

  • 国家 US

  • 入库时间 2022-08-21 18:54:51

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号