首页> 外国专利> TITANIUM GROUP ELEMENT BASED FLUORINE ADSORBING-DESORBING AGENT FOR FLUORINE-CONTAINING PROCESS LIQUID TREATMENT FOR WET ZINC SMELTING, AND METHOD FOR REMOVING FLUORINE

TITANIUM GROUP ELEMENT BASED FLUORINE ADSORBING-DESORBING AGENT FOR FLUORINE-CONTAINING PROCESS LIQUID TREATMENT FOR WET ZINC SMELTING, AND METHOD FOR REMOVING FLUORINE

机译:基于钛族元素的氟吸附解吸剂用于湿法炼锌的含氟过程液及去除氟的方法

摘要

PROBLEM TO BE SOLVED: To provide a titanium group element based fluorine adsorbing-desorbing agent for fluorine-containing process liquid treatment for wet zinc smelting which does not increase equipment cost, running cost or the like, and with which process control is facilitated, and to provide a method for removing fluorine.;SOLUTION: Using a titanium group element based compound selected from titanium, zirconium and hafnium as a fluorine adsorbing-desorbing agent, in a fluorine adsorbing stage, fluorine is adsorbed into the fluorine adsorbing agent, and, in a fluorine desorbing stage, the adsorbed fluorine is desorbed, and is reused as a fluorine adsorbing-desorbing agent. In the fluorine desorbing process, the value of the ratio between the content of the fluorine contained in the process liquid for wet zinc smelting and the content of the titanium group element contained in the titanium group element based compound to be contacted, [(the titanium group element content: mg/L)/(the fluorine content: mg/L)] is controlled to 20 to 600, a satisfactory contact state is maintained, and they are contacted for about 30 min.;COPYRIGHT: (C)2010,JPO&INPIT
机译:解决的问题:提供一种用于湿式锌熔炼的含氟处理液处理的钛族元素基氟吸附解吸剂,其不增加设备成本,运行成本等,并且有助于进行工艺控制,并且提供一种去除氟的方法。解决方案:使用选自钛,锆和ha的钛族元素基化合物作为氟吸附解吸剂,在氟吸附步骤中,将氟吸附到氟吸附剂中,然后,在氟的解吸阶段,吸附的氟被解吸,并再次用作氟吸附-解吸剂。在氟解吸工序中,湿式锌冶炼用处理液中所含的氟的含量与所接触的钛族元素系化合物中所含的钛族元素的含量之比的值[[(钛族元素含量:mg / L)/(氟含量:mg / L)]控制在20至600,保持令人满意的接触状态,并接触约30分钟。版权所有:(C)2010,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号