A copper recovery process comprising the steps of: a) providing (200) a material containing copper sulfide; b) shred (202) said material containing copper sulphide to obtain a shredded material containing copper sulphide in sludge form; c) subjecting said sludges to a flotation (208) to separate materials containing copper sulfide and forming (210) a concentrated material containing copper sulphide; d) pressure leaching (220) of said concentrated material containing copper sulphide, at a temperature in the range of 210 ° C to 235 ° C in an oxygen-containing atmosphere, in a sealed pressure vessel of agitated leaching of multiple compartments, to form a product sludge; e) separating (228) said product sludge in a solution containing copper and a residue (280) containing solids; f) adjust the pH value of said copper-containing solution to a pH value lower than 2.2 by chemical adjustment (232) and combining said copper-containing solution with a dilution solution (250) to obtain a solution that it contains copper with adjusted pH, where the ratio between said solution containing copper and said dilution solution is in the range between 1: 4 to 1: 8; g) solvent extraction (252) and electrolytic extraction (254) of said adjusted pH solution containing copper to obtain a refined solution (260) and a copper cathode; h) applying said refining solution containing the acid to a heap leaching operation (262).
机译:一种铜的回收方法,包括以下步骤:a)提供(200)含有硫化铜的材料; b)切碎(202)所述含硫化铜的材料以获得含淤渣形式的硫化铜的切碎的材料; c)将所述污泥进行浮选(208)以分离含有硫化铜的材料,并形成(210)含有硫化铜的浓缩材料; d)在密封的压力容器中,在多个隔室中搅拌浸出,在210℃至235℃的温度下,在210℃至235℃的温度范围内,对所述含硫化铜的浓缩材料进行加压浸出(220),以形成产品污泥; e)在含铜的溶液和含固体的残余物(280)中分离(228)所述产物污泥; f)通过化学调节(232)将所述含铜溶液的pH值调节至低于2.2的pH值,并且将所述含铜溶液与稀释溶液(250)合并以获得溶液,其中所述溶液包含经调节的pH的铜,其中所述含铜溶液与所述稀释溶液的比例在1:4至1:8之间; g)所述的含有铜的调节pH溶液的溶剂萃取(252)和电解萃取(254),以获得精制溶液(260)和铜阴极; h)将所述包含酸的精制溶液施用于堆浸操作(262)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号