首页> 外国专利> Cobalt recovery method and nickel from laterite ore by a combination of medium-leaching and atmospheric pressure leaching

Cobalt recovery method and nickel from laterite ore by a combination of medium-leaching and atmospheric pressure leaching

机译:中浸与大气压浸结合回收红土矿石中钴和镍的方法

摘要

It is a procedure for leaching laterite ore containing limonite and saprolite. Sufficient inorganic acid is added to the limonite slurry, it is leached at atmospheric pressure, which dissolves the soluble iron soluble and non-ferrous metals of majority. After addition of saprolite at a pressure above atmospheric pressure and temperatures above the normal boiling point further, the slurry sufficient to leach the majority of the nickel contained in the saprolite, and to precipitate most of the iron in solution The brewing time is. Pressure of the slurry is then decreased, nickel and / or cobalt solvent extraction continues, resin - in - ion exchange or other pulp method, by recovery or other methods of hydroxide precipitation, or sulfide, is recovered from the leachate that.
机译:这是一种浸出含褐铁矿和腐泥土的红土矿石的程序。将足够的无机酸添加到褐铁矿浆中,在大气压下将其浸出,从而溶解了大部分可溶性铁和非铁金属。在高于大气压的压力和高于正常沸点的温度下添加腐泥土后,浆液足以浸出腐泥土中所含的大部分镍,并使溶液中的大部分铁沉淀。酿造时间为。然后降低浆料的压力,继续进行镍和/或钴溶剂的萃取,通过回收或通过其他方法回收氢氧化物沉淀或硫化物,从渗滤液中回收树脂-离子交换或其他纸浆方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号