PREPARATION METHOD OF TWO-PHASE CARBON NANOFIBERS AND ACTIVATED CARBON NANOFIBERS BY ELECTROSPINNING FROM POLYACRYLONITRILE/PITCH BLEND SOLUTIONS

机译:聚丙烯腈/沥青混合溶液电纺丝制备两相碳纳米粉和活性炭纳米粉

摘要

A method for manufacturing two-component carbon nanofibers and activated carbon nanofibers is provided to increase specific surface areas of the carbon nanofibers and improve electrical conductivity of the carbon nanofibers, and usefully apply the carbon nanofibers to electrode materials, adsorbing materials, and carbon fiber fillers for composite materials. A spinning solution is prepared by dissolving PAN(polyacrylonitrile) and pitch, as carbon fiber precursors, into an organic solvent solution selected from THF(tetrahydrofuran), DMF(dimethylformamide), DMAc(dimethylacetamide), pyridine, and quinoline. A high voltage is applied to the spinning solution to produce organic nanofibers having radii of 0.1-0.9um through electrospinning. The organic nanofibers are oxidation-stabilized to produce flameproof fibers using air. The flameproof fibers are carbonized, activated, or graphitized to produce carbon nanofibers, activated carbon nanofibers, or graphite carbon nanofibers.
机译:提供了一种用于制造两组分碳纳米纤维和活性碳纳米纤维的方法,以增加碳纳米纤维的比表面积并改善碳纳米纤维的电导率,并且有用地将碳纳米纤维应用于电极材料,吸附材料和碳纤维填料。用于复合材料。通过将PAN(聚丙烯腈)和沥青(作为碳纤维前体)溶解在选自THF(四氢呋喃),DMF(二甲基甲酰胺),DMAc(二甲基乙酰胺),吡啶和喹啉的有机溶剂溶液中,制备纺丝溶液。通过电纺丝向纺丝溶液施加高压以生产半径为0.1-0.9um的有机纳米纤维。使用空气将有机纳米纤维氧化稳定以生产防火纤维。将耐火纤维碳化,活化或石墨化以产生碳纳米纤维,活性碳纳米纤维或石墨碳纳米纤维。

著录项

  • 公开/公告号KR100759102B1

    专利类型

  • 公开/公告日2007-09-19

    原文格式PDF

  • 申请/专利权人 NANO TECHNICS CO. LTD.;

    申请/专利号KR20060048153

  • 发明设计人 KIM CHAN;KIM YOUNG MIN;

    申请日2006-05-29

  • 分类号D01F9/12;D01F9/22;

  • 国家 KR

  • 入库时间 2022-08-21 20:31:22

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号