PROBLEM TO BE SOLVED: To effectively eliminate the unevenness of erosion of a refractory in the state of scarcely needing the investment of an equipment and to prolong the service life of furnace body in a converter by disposing plural oxygen spouting holes asymmetrically to the center axis of a lance and displacing the lance by a prescribed angle around the center axis according to the erosion of the lining refractory in the converter. ;SOLUTION: In the converter 1 covering the outermost shell with an iron shell 8 and lining the lining refractory 7 in the converter at the inside of the iron shell, oxygen is blown as gaseous oxygen jet 6 from a top-blown lance 5 and molten steel 3 and molten slag 4 are vigorously stirred to execute the active combustion action of carbon. At this time, since the lining refractory 7 is unevenly eroded by the high temp. generated with the combustion of the carbon and the erosion with the molten slag 4, the oxygen spouting holes 5a arranged at the tip part of the lance 5 are asymmetrically disposed. Then, the lance 5 is displaced by rotating so as to direct the direction where the oxygen jet intensity of the lance 5 is weak to the position having large erosion in the furnace based on the information in the furnace, and during blowing, the lance 5 is fixed.;COPYRIGHT: (C)2000,JPO
机译:要解决的问题:通过在与炉膛中心轴线不对称的位置设置多个氧气喷出孔,在几乎不需要设备投资的状态下有效消除耐火材料侵蚀的不均匀性,并延长转炉中炉体的使用寿命。喷枪,并根据转炉中炉衬耐火材料的腐蚀,使喷枪围绕中心轴线以规定的角度移动。 ;解决方案:在转炉1中,用铁壳8覆盖最外壳并在炉壳内的耐火材料内衬上衬里耐火材料7,将氧气作为气态氧气射流6从顶吹喷枪5吹入并熔融剧烈搅拌钢3和熔渣4以执行碳的主动燃烧作用。此时,由于耐火材料7被高温不均匀地侵蚀。由于碳的燃烧和熔渣4的侵蚀而产生的氧,布置在喷枪5的尖端部分的氧气喷出孔5a不对称地设置。然后,喷枪5通过旋转而移位,以基于炉中的信息将喷枪5的氧气喷射强度弱的方向引导到炉中具有较大侵蚀的位置,并且在吹塑期间喷枪5是固定的。;版权:(C)2000,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号