PURPOSE: Provided are a cement admixture with high strength, low shrinkage and low temperature application, and a cement composition with much improved initial strength, longtime strength and durability compared with portland cement by mixing cement with the prepared admixture. CONSTITUTION: The admixture comprises 75-100wt.% Al2(SO4)3 as a main material, 0-10wt.% of Na2CO3, 0-10wt.% of NaAlO2, 0-25wt.% of CaCl2, 0-15wt.% of limestone, and 0-5wt.% of magnesium fluosilicate, where the all materials have a specific surface area of 2000cm¬2/g or more, except limestone with a specific surface area of 5000cm¬2/g or more. Also, the cement admixture is prepared by adding 1-10wt.% of the prepared admixture to conventional cement such as portland cement, high early-strength portland cement, fly ash cement or blast furnace slag cement.
机译:目的:提供了具有高强度,低收缩性和低温应用的水泥掺合料,以及通过将水泥与制备的掺合料相混合而与波特兰水泥相比具有大大改善的初始强度,长期强度和耐久性的水泥组合物。组成:该混合物包含75-100wt。%的Al2(SO4)3作为主要材料,0-10wt。%的Na2CO3、0-10wt。%的NaAlO2、0-25wt。%的CaCl2、0-15wt。%的Al石灰石和0-5wt。%的氟硅酸镁,其中所有材料的比表面积都为2000cm2 / g或更高,石灰石的比表面积为5000cm2 / g或更高。另外,通过将1-10wt。%的制备的混合物添加到常规水泥例如波特兰水泥,高早强波特兰水泥,粉煤灰水泥或高炉矿渣水泥中来制备水泥混合物。

著录项

  • 公开/公告号KR100508207B1

    专利类型

  • 公开/公告日2005-08-17

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20010021565

  • 发明设计人 박응모;문경주;

    申请日2001-04-20

  • 分类号C04B22/14;

  • 国家 KR

  • 入库时间 2022-08-21 22:03:33

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号