The invention is WGS inorganic elastic coating material capable of enhancing the strength of concrete surfaces, wood, acts with the surface of the water and is applied to the surface of the glass and chemicals protect the structure or product from deterioration and aging of concrete structures - PCC ( WGS - relates to a coating method using the same construction of the structure surface and a process for producing a Polymer Ceramics coating).; The inorganic elastic coating when a coating material is prepared by hydration reaction of a modified synthetic polymer water-soluble polymer and cement in minerals, in particular applying the coating material to the surface of the concrete structure to neutralize the acidic cement harmful environmental hormones to the environment It can be varied in nature friendly concrete structures that do not discharge, and also when applied to underwater concrete structures to prevent the external sea water which penetrates into the concrete structure, consequently preventing salt damage and deterioration of the concrete structure in water.; Method for producing the coating material is a first step of steam and dispersing material, and start again with a formulation manufactured into water with a stirrer to prepare a formulation by stirring while heating up to degrees of 80 degrees, and in the second step in the first step separate after then placed in a tank may medium and a dispersing agent and re-adding the start material and water with stirring after each addition of a plurality of monomers that have different functions to prepare a formulation as a third step of the formulation prepared in the second step for a while to cool the ammonia and liquid form into water consisting of modified acrylic water-soluble polymer prepared by dropping an additive formulation, and at the same time of the WGS-PCC B first with normal cement, fly ash, half of gypsum, cellulose fiber, and other admixtures by blending the formulation of a powdered WGS-PCC a first prepared as mixed with a constant mixing ratio by weight of the by hydration reaction It will cost.; Construction method for coating the surface of the structure by using the above prepared inorganic elastic coating material is as follows.; First, when the surface of the structure in dry condition; Determining a portion that requires the status and the overall structure of the coating; Filling surface voids and cleanup sites for parts which require a coating on the surface of the structure; Applying a reinforcing agent to the WGS-Real surface structure surface; Applying to the mineral resilient coating; And through the step of curing at a given time or a coating method on the surface of the dry structure consisting of checking the quality of the coating.; Alternatively, the surface is a wetting surface with the water of the structure or if it is a leak occurs, the surface of; Determining a portion that requires the status and the overall structure of the coating; Clean surface of a portion that requires a coating on the surface of the structure and leakage site cleanup phase; Selecting one of the WGS water gongbeopin front, filling, a back or composite waterproofing grouting method of the leak portion on the structure surface and subjected to block the leakage grouting; And clean the surface of the structure step to clean a surface; Applying to the WGS-Real surface reinforcing agent; Applying to the polymer-based inorganic coating; And a coating method for a surface of the structure resulting wet or leaking after the step of checking the quality of the coatings through a step of curing at a given time.
机译:本发明是WGS无机弹性涂料,能够增强混凝土表面,木材的强度,与水的表面作用并应用于玻璃表面,化学药品可保护结构或产品免受混凝土结构的老化和老化- PCC(WGS-涉及使用与结构表面相同的构造的涂覆方法以及生产聚合物陶瓷涂层的方法)。当通过改性合成聚合物水溶性聚合物和水泥在矿物中的水合反应制备涂料时,无机弹性涂料,特别是将涂料施用于混凝土结构表面以中和酸性水泥有害的环境激素。环境在不排放的自然友好型混凝土结构中,以及在应用于水下混凝土结构时,可以防止外部海水渗入混凝土结构,从而防止盐分破坏和水中混凝土结构的变质,从而改变环境。制备涂料的方法是第一步,将物料蒸汽分散,然后再次用搅拌器将制剂制成水,然后在加热至80度的同时进行搅拌来制备制剂,然后进行第二步第一步分离,然后将其放入罐中,然后将介质和分散剂放入容器中,并在每次添加多种具有不同功能的单体后,在搅拌下重新加入原料和水,以制备制剂,作为制备制剂的第三步在第二步中将氨和液体形式冷却到由滴加添加剂配方制成的改性丙烯酸水溶性聚合物组成的水中,同时首先将WGS-PCC B与普通水泥,粉煤灰混合,通过混合粉末状WGS-PCC的配方将一半的石膏,纤维素纤维和其他掺合料混合在一起反应这将花费。使用上述制备的无机弹性涂料涂覆结构表面的方法如下。首先,当结构表面处于干燥状态时;确定需要涂层状态和整体结构的部分;填充需要在结构表面上进行涂层的零件的表面空隙和清理位置;在WGS-Real表面结构表面上施加增强剂;适用于矿物弹性涂料;并通过在给定时间固化的步骤或在干燥结构表面上的涂覆方法来检查涂层的质量。或者,该表面是用该结构的水润湿的表面,或者如果发生泄漏,则是该表面;确定需要涂层状态和整体结构的部分;清洁需要在结构表面上进行涂层和泄漏部位清理阶段的部分表面;选择WGS水工拱顶面在结构表面上的渗漏部位的正面,填充,背面或复合防水灌浆方法之一,并对渗漏浆进行堵漏;并清洗结构表面的步骤以清洗表面;适用于WGS-Real表面增强剂;适用于聚合物基无机涂料;以及一种用于在给定时间通过固化步骤检查涂层质量的步骤之后导致湿润或渗漏的结构表面的涂覆方法。

著录项

  • 公开/公告号KR20050077928A

    专利类型

  • 公开/公告日2005-08-04

    原文格式PDF

  • 申请/专利权人 W G S CO. LTD.;CHOI CHOON SIK;

    申请/专利号KR20040005616

  • 发明设计人 CHOI CHOON SIK;

    申请日2004-01-29

  • 分类号C09D1/08;

  • 国家 KR

  • 入库时间 2022-08-21 22:04:48

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号