摘要

PURPOSE: Provided are a modified synthetic asphalt containing styrene-butadiene-rubber latex and gilsonite, a method for preparing the same, and a method for producing a modified synthetic asphalt concrete containing the same. CONSTITUTION: The modified synthetic asphalt comprises 90-94 wt% of AC 60-70 or AC 85-100(based on domestic invasion) normal aspha 4-2 wt% of styrene-butadiene-rubber(SBR) latex having solids of 40-50%; and 6-4 wt% of gilsonite. The asphalt is prepared by the steps of (i) introducing 90-94 wt% of liquefied asphalt into mixing tank; (ii) introducing 4-6 wt% of gilsonite liquid or powder into the mixing tank; (iii) introducing 2-4 wt% of styrene-butadiene-rubber latex having solids of 40-50% into the mixing tank by atomizing; and (iv) evaporating the remaining moisture from the mixing tank.
机译:目的:提供一种含有苯乙烯-丁二烯-橡胶胶乳和硅灰石的改性合成沥青,其制备方法以及生产含有它们的改性合成沥青混凝土的方法。组成:改性合成沥青包含90-94 wt%的AC 60-70或AC 85-100(基于国内入侵)普通沥青; 4-2重量%的固体含量为40-50%的苯乙烯-丁二烯-橡胶(SBR)胶乳;和6-4 wt%的硅灰石。所述沥青通过以下步骤制备:(i)将90-94wt%的液化沥青引入混合罐中; (ii)将4-6重量%的硅灰石液体或粉末引入混合槽中; (iii)通过雾化将2-4重量%的固体含量为40-50%的苯乙烯-丁二烯-橡胶胶乳引入混合罐中; (iv)蒸发混合罐中剩余的水分。

著录项

  • 公开/公告号KR100435848B1

    专利类型

  • 公开/公告日2004-06-10

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20000064871

  • 发明设计人 황성도;유성열;안신환;

    申请日2000-11-02

  • 分类号C08L95/00;

  • 国家 KR

  • 入库时间 2022-08-21 22:46:57

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号