首页> 外国专利> Method to eliminate weld solidification cracking of 312 stainless steel overlay and to minimize the overlay's thermal expansion mismatch with carbon steel or low alloy steel substrate

Method to eliminate weld solidification cracking of 312 stainless steel overlay and to minimize the overlay's thermal expansion mismatch with carbon steel or low alloy steel substrate

机译:消除312不锈钢表层的焊接凝固裂纹并最小化表层与碳钢或低合金钢基材的热膨胀不匹配的方法

摘要

A method for applying a stainless steel weld overlay on a substrate, e.g., a carbon steel or low alloy steel, uses an arc welding process. The process includes welding a stainless steel weld overlay onto the substrate using a shielding gas mixture including greater than 2% nitrogen by volume with balance being an inert gas or a mixture of inert gases. The nitrogen is of a sufficient concentration so as to eliminate solidification cracking in the weld overlay. In addition, the nitrogen may help to eliminate a mismatch in me coefficient of thermal expansion between the weld overlay and the substrate. Furthermore, if the weld overlay comprises only a single layer, the nitrogen concentration in the shielding gas mixture may be less than 2%.
机译:将电弧焊工艺施加在例如碳钢或低合金钢的基底上的不锈钢堆焊层的方法。该方法包括使用保护气体混合物将不锈钢焊缝堆焊在基底上,该保护气体混合物包含大于2%(体积)的氮气,其余为惰性气体或惰性气体的混合物。氮的浓度足以消除焊缝中的凝固裂纹。此外,氮气可以帮助消除焊缝覆盖层和基材之间的热膨胀系数不匹配。此外,如果焊缝覆盖层仅包括单层,则保护气体混合物中的氮浓度可以小于2%。

著录项

  • 公开/公告号US6204477B1

    专利类型

  • 公开/公告日2001-03-20

    原文格式PDF

  • 申请/专利权人 WSI WELDING SERVICES INC.;

    申请/专利号US19970002119

  • 发明设计人 GEORGE YING-DEAN LAI;

    申请日1997-12-31

  • 分类号B23K90/00;

  • 国家 US

  • 入库时间 2022-08-22 01:04:52

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号