首页> 外国专利> Method of leaching Gold by cyanide leaching of Refractory ores or Concentrates, in which the gold is as tellurides and comprising deliver air at Atmospheric Pressure.At a temperature of 60 degrees Celsius and a value immediately below the Boiling Point of the liquid at a high pH of leaching and 10 to 12.

Method of leaching Gold by cyanide leaching of Refractory ores or Concentrates, in which the gold is as tellurides and comprising deliver air at Atmospheric Pressure.At a temperature of 60 degrees Celsius and a value immediately below the Boiling Point of the liquid at a high pH of leaching and 10 to 12.

机译:通过氰化物浸出难熔矿石或精矿而浸出金的方法,其中金为碲化物,包括在大气压下输送空气。温度为摄氏60度,在高pH下其值刚好低于液体的沸点浸出和10到12。

摘要

The Invention relates to a method to enhance the performance of Gold leaching by cyanidation In Treatment of Refractory ores or concentrates of such MineThe Air Delivery, while in an Alkaline Environment at Atmospheric Pressure, in which the Gold present in such ores or concentrates is fixed as teleruros.The method is characterized by making the cyanide to a temperature above the Ambient temperature.Until a value immediately below the Boiling Point of liquid leaching. The treatment is performed appropriately at a temperature of 60 to 80 degrees C.And a pH value between 10 and 12.
机译:本发明涉及一种通过氰化来提高金的浸出性能的方法,该方法在大气中的碱性环境中在大气中将存在于所述矿石或精矿中的金固定为空气时,通过在此类矿山的难处理矿石或精矿中的空气输送进行处理。该方法的特征是使氰化物达到高于环境温度的温度,直到其值刚好低于液体浸出的沸点。在60到80摄氏度的温度和10到12的pH值之间适当地进行处理。

著录项

  • 公开/公告号CL2000003176A1

    专利类型

  • 公开/公告日2001-10-11

    原文格式PDF

  • 申请/专利权人 BOLIDEN MINERAL AB;

    申请/专利号CL2000003176

  • 发明设计人 JAN-ERIC SUNDKVIST;

    申请日2000-11-16

  • 分类号C22B11/08;C22B3/12;

  • 国家 CL

  • 入库时间 2022-08-22 01:25:50

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号