PROBLEM TO BE SOLVED: To obtain an asphalt pavement binder capable of decreasing road surface pickup by mixing an asphalt cement, a crumb rubber and a specific polyoctenamer. SOLUTION: After 80-99 mass % (hereafter ms.%), preferably 80-95 ms.% asphalt cement, based on the total mass of a composition is heated in the range of 137.8-176.7 deg.C 0.5-20 ms.%, preferably 2-15 ms.% crumb rubber and 0.01-10 ms.%, preferably 0.2-5 ms.% trans-polyoctenamaer rubber, in which about 80%, preferably 60% double bond, is in trans-position and the melting point is 45 deg.C, preferably 30 deg.C, are mixed. Subsequently the asphalt cement and the crumb rubber are homogeneously dissolved in the polyoctenamer by heating and mixing to produce the binder composition.
机译:要解决的问题:通过混合沥青水泥,碎橡胶和特定的聚辛烯来获得能够减少路面拾取的沥青路面粘合剂。解决方案:在80-99质量%(此后为ms。%),优选80-95 ms。%的沥青水泥之后,基于组合物的总质量在137.8-176.7℃范围内加热0.5-20 ms。 %,优选2-15ms。%的碎屑橡胶和0.01-10ms。%,优选0.2-5ms。%的反式聚辛烯橡胶,其中约80%,优选60%的双键处于转位,并且混合熔点为45℃,优选30℃。随后,通过加热和混合将沥青水泥和碎屑橡胶均匀地溶解在聚辛烯单体中以产生粘合剂组合物。

著录项

  • 公开/公告号JP2000119530A

    专利类型

  • 公开/公告日2000-04-25

    原文格式PDF

  • 申请/专利权人 DEGUSSA HUELS AG;

    申请/专利号JP19990295596

  • 发明设计人 BURNS BERNARD J;

    申请日1999-10-18

  • 分类号C08L95/00;C08L21/00;E01C7/26;

  • 国家 JP

  • 入库时间 2022-08-22 01:59:47

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号