首页> 外国专利> METHOD FOR MEASURING THICKNESS OF SOLIDIFIED SHELL IN CONTINUOUS CASING AND INSTRUMENT THEREFOR

METHOD FOR MEASURING THICKNESS OF SOLIDIFIED SHELL IN CONTINUOUS CASING AND INSTRUMENT THEREFOR

机译:连续套管中凝固壳厚度的测定方法及其仪器

摘要

PROBLEM TO BE SOLVED: To enable the accurate measurement of solidified shell in a mold by calculating the increasing part of the solidified shell thickness at a tracing point based on conductive heat flux and the solidified shell thickness just before generating this conductive heat flux, using the increasing part of the solidified shell and drawing-out speed and repeatedly renewing the solidified shell thickness and the position of the tracing point. ;SOLUTION: Molten metal 3 is cooled in the mold 1 arranging thermocouples 2 and continuously drawn out with pinch rolls 5 while forming the solidified shell 4. The molten metal surface level 7, i.e., solidified starting point is measured with a molten metal surface level meter 6. A detecting instrument 8 makes the data of mold temp., the molten metal surface level 7, drawing-out speed and cooling water temp., and gives to an arithmetic device 9, and the distribution of the solidified shell thickness in the mold is displayed on a displaying device 10. According to a prescribed process, the decision of the tracing point of calculating objection of the solidified shell 4 thickness, the conductive heat flux at the tracing point, the solidified shell 4 thickness and drawing-out speed are measured in the real time. By this method, the abnormal operation is detected at early time, and the quality of continuously cast slab and the productivity can be improved.;COPYRIGHT: (C)1998,JPO
机译:要解决的问题:为了在模具中精确测量凝固的壳体,可以在生成导电热通量之前,根据传导热通量和凝固的壳体厚度,在示踪点计算凝固的壳体厚度的增加部分,从而精确测量模具中的凝固壳体。增加凝固壳的部分和抽出速度,并反复更新凝固壳的厚度和追踪点的位置。 ;解决方案:熔融金属3在装有热电偶2的模具1中冷却,并在形成凝固壳4的同时用夹送辊5连续抽出。熔融金属表面水准7(即凝固起始点)是用熔融金属表面水准测量的检测仪器8检测模具温度,熔融金属表面液位7,抽出速度和冷却水温度的数据,并将其提供给算术装置9,并且将凝固壳厚度在测量仪中的分布。模具被显示在显示装置10上。根据规定的过程,决定计算凝固壳4的厚度的对象的追踪点,在该凝固点处的热传导率,凝固壳4的厚度和抽出速度。是实时测量的。通过这种方法,可以及早发现异常运行情况,提高连铸坯的质量,提高生产效率。;版权所有:(C)1998,日本特许厅

著录项

  • 公开/公告号JPH10277716A

    专利类型

  • 公开/公告日1998-10-20

    原文格式PDF

  • 申请/专利权人 NIPPON STEEL CORP;

    申请/专利号JP19970082901

  • 发明设计人 SUZUKI NORIYUKI;

    申请日1997-04-01

  • 分类号B22D11/16;

  • 国家 JP

  • 入库时间 2022-08-22 03:08:29