PURPOSE: To produce the corrosion resistant aluminum bronze alloy improved in hot expandability by imparting the hot expandability equiv. to the hot expandability of an α+β two-phase alloy to this aluminum bronze alloy even if the alloy has the corrosion resistance equiv. to the corrosion resistance of an α single phase aluminum bronze. ;CONSTITUTION: This aluminum alloy contains, by weight, 3 to 8% Al and 1 to 5% Si and either or both of 0.2 to 3% components of either one or two kinds of Sn and Cr or 0.2 to 3% of components of either one or two kinds of Pb and Ni an addition to these Al and Si components and consists of the balance Cu and incidental inevitable impurities. The excellent expandability of this alloy causes the two phases α+β at a hot expanding temp. (700 to 800°C). In addition, the alloy in the α single phase at ≤650°C service temp. and, therefore, the alloy exhibits the corrosion resistance of the α single phase aluminum bronze in the ordinary service temp. region. This alloy is optimal for use in parts for high-temp. corrosion resistance to be produced by using an expansion method, such as precision casting and hot extruding.;COPYRIGHT: (C)1994,JPO
机译:目的:通过赋予等价的热膨胀性来生产耐腐蚀的铝青铜合金,其热膨胀性得到改善。 α+β两相合金对铝青铜合金的热膨胀性,即使该合金具有同等的耐蚀性。 α单相铝青铜的耐腐蚀性。 ;组成:该铝合金按重量计包含3%至8%的Al和1%至5%的Si,以及0.2到3%的一种或两种Sn和Cr成分之一或两者,或0.2到3%的一种或两种成分这些Al和Si成分中除了Pb和Ni以外,还包含一种或两种,并且由余量的Cu和不可避免的杂质组成。这种合金极好的膨胀性使两相α+β处于热膨胀温度。 (700至800°C)。此外,α单相合金在≤650°C的使用温度下。因此,该合金在正常使用温度下具有α单相铝青铜的耐腐蚀性。地区。这种合金是用于高温零件的最佳选择。通过膨胀方法,如精密铸造和热挤压生产,具有良好的耐腐蚀性。;版权所有:(C)1994,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号