A thermally-reactive, sprayable hot-melt adhesive (I) contains a mixt. of polycaprolactone (II) and solid phthalate ester (III). Pref. mixt. (I) contains 40-65 (pref. 50) wt.% polyester, pref. a polycaprolactone-based polyester resin with mol.wt. 45,000-55,000 and m.pt. 59-62 deg.C (II), and 35-60 (pref.50) wt.% (III), pref. a phthalate plasticiser of the dicyclohexyl phthalate type. USE/ADVANTAGE - Used for spraying at working temps. of at least 120 (pref. 120-140) deg.C, esp. for coating uneven, irregular surfaces and for contactless application on leather, paper and textiles, and for rated breaking pts. at 70 deg.C (claimed). W.r.t. conventional hot melts (e.g. EVA copolymer compsns.), (I) has a much longer open time (10 mins. compared with about 45 secs.) and can be sprayed at temps. of 120-140 deg.C, compared with above 150 deg.C for prior-art compsns.; (I) enables good adhesion on `difficult' substrates, and (because of its low m.pt., e.g. 70 deg.C) does not have to be kept under inert gas before us
机译:热反应性,可喷涂的热熔粘合剂(I)包含混合物。聚己内酯(II)和固体邻苯二甲酸酯(III)的制备。首选混音(I)包含40-65(优选50)重量%的聚酯,优选。 mol.wt.的聚己内酯基聚酯树脂。 45,000-55,000和m.pt. 59-62℃(II)和35-60(优选50)wt。%(III),优选邻苯二甲酸二环己基酯类的邻苯二甲酸酯增塑剂。使用/优点-用于在工作温度下喷涂。至少120(摄氏120-140)摄氏度,尤其是用于涂覆不平整,不规则的表面,以及在皮革,纸张和纺织品上的非接触式应用,以及用于额定断裂点。在70摄氏度(声称)。 。常规的热熔体(例如,EVA共聚物组合物),(I)具有更长的开放时间(10分钟,而约45秒),并且可以在一定温度下喷雾。 120-140℃,而现有技术的组合物高于150℃; (I)能够在'困难'的基材上实现良好的附着力,并且(由于其较低的熔点,例如70摄氏度)不必在我们面前保持惰性气体

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号