1. The invention concerns a leaching method for oxidised zinciferous materials, particularly for roasted sphalerite, by means of sulfur acid solution, whereas the materials are supplied continuously by means of a worm conveyor, whereas in the tubular part of worm conveyor oxidised zinciferous materials are mixed with reverse electrolyte from zinc electrolysis while maintaining the ratio of oxidised zinciferous materials to reverse electrolyte preferably at 1:8 be volume and up to 90 percent of H2SO4 amount as necessary for dissolving zinc oxide comprised in leached zinciferous materials, and then the pulp so formed is directed to a passage tank where zinciferous materials and the sulfur acid and zinc sulfate are further mixed, and then from the passage tank, the pulp is collected and directed for further leaching, characterised in that roasted sheet zinc preferably in the form of mixture of roasted ore from grains and dusts is subject to conditioning at temperature preferably from 260 to 170 degrees Celsius for 2-4 hours in a closed space, and then the roasted ore from grains and dusts is subject to stirring in the worm conveyor if necessary, or the mixture of roasted ore from threshold and dusts is directed through the worm conveyor to a worm gear feeder, and finally to the tubular outlet where the roasted sphalerite is subject to leaching in a tubular head.IMAGE
机译:本发明涉及一种氧化的含锌材料,特别是用于焙烧闪锌矿的浸出方法,其通过硫酸溶液,而该材料是通过蜗杆输送机连续供应的,而在蜗杆输送机的管状部分中,氧化的含锌材料是连续的。与锌电解中的反电解液混合,同时保持氧化的含锌材料与反电解液的比例优选为1:8的体积,并需要最多90%的H2SO4量,以溶解浸出的含锌材料中所含的氧化锌,然后将其制成纸浆所形成的被引导至通槽,在此处将含锌材料与硫酸和硫酸锌进一步混合,然后从通槽中收集纸浆并引导以进一步浸出,其特征在于,烤制的锌片优选为混合物形式来自谷物和粉尘的焙烧矿石要进行温度调节,最好为260°C密闭空间中在170摄氏度下加热2-4小时,然后根据需要在蜗杆输送机中搅拌谷物和粉尘的焙烧矿石,或者将门槛和粉尘的焙烧矿石的混合物引导通过蜗杆输送机到蜗轮进料器,最后到管状出口,经过烘烤的闪锌矿在管状头中浸出。<图像>

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号