Method of reducing the percentage of Alumina Trihydrate Crystals with diameter less than 200 microns.Comprising: (a) add the liquid to the procedure before the crystallization of Bayer Alumina Trihydrate, 50 ppm of a Poly (Acid crilico); (b) to treat the mixture of between 65 and 79jc) for 15 to 20 hours to precipitate the large Crystals of Alumina Trihydrate; (c) add to aliquido ago The Bayer Process (60 ppm of Poly (acrylic acid)To agglomerate Sodium oxalate crystals; (d) add to the Mix (c) seed Crystals of Sodium oxalate; and (e) to cool The Liquid Crystallizer temperature enough, for all the Sodium oxalate. It is used to purify the alumina.
机译:减少直径小于200微米的三水合氧化铝晶体百分比的方法。包括:(a)在拜耳三水合氧化铝结晶之前,向该程序中添加50 ppm的聚(酸性cricrico)溶液; (b)处理65至79℃之间的混合物15至20小时,以沉淀出三水合氧化铝的大晶体; (c)添加到aliquido之前的拜耳法(60 ppm的聚(丙烯酸)聚结成草酸钠结晶;(d)添加到混合物(c)草酸钠的晶种中;和(e)冷却液晶结晶器温度足够高,可以吸收所有草酸钠,用于纯化氧化铝。

著录项

  • 公开/公告号ES8707871A1

    专利类型

  • 公开/公告日1987-11-16

    原文格式PDF

  • 申请/专利权人 NALCO CHEMICAL COMPANY;

    申请/专利号ES19860554032

  • 发明设计人

    申请日1986-04-16

  • 分类号B01D9/00;C08F120/06;

  • 国家 ES

  • 入库时间 2022-08-22 06:57:19

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号