A method of heat treating a component formed of a high-chromium cast ferrous-based alloy consisting of 11-28 wt% chromium, 1 - 3.6 wt% carbon and at least 0.2 wt% molybden um and/or at least 0.6 wt% tungsten, the remainder (apart from any incidental ingredients and impurities) being iron, said method comprising the steps of:-;a) holding said component at a temperature between the solidus temperature of the alloy and 1050°C for a period of time not exceeding 3 days in a non-oxidising atmosphere or vacuum so as to produce a partially spheroidised hard carbide phase in an austenitic matrix throughout the component, and;b) quenching the component at a mean rate of from 40'C/min to 3'C/min in the critical temperature range in order to retain the austenitic matrix.;Before heat treatment, carbon and chromium form a hard sharp, angular carbide phase and the molybdenum and/or tungsten serves to increase the rate of change in the morphology of the carbide phase during heat treatment from sharp angularity to a partly spheroidised morphology.
机译:一种对由高铬铸造的铁基合金形成的部件进行热处理的方法,该合金由11-28 wt%的铬,1-3.6 wt%的碳和至少0.2 wt%的钼和/或至少0.6 wt%的钨组成其余的(除任何偶然的成分和杂质之外)是铁,所述方法包括以下步骤:-; a)将所述组分在合金的固相线温度和1050°C之间的温度下保持不超过一段时间在非氧化性气氛或真空中放置3天,以便在整个组件中的奥氏体基体中产生部分球化的硬质碳化物相;并且; b)以40'C / min至3'C的平均速率淬灭组件/ min在临界温度范围内,以保留奥氏体基体。在热处理之前,碳和铬形成硬而尖锐的角质碳化物相,而钼和/或钨则可提高合金形态的变化率。尖锐的a热处理过程中的碳化物相局部性为球形。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号