METHOD FOR THERMALLY REFORMING COAL HAVING LOW RANK OF COALIFICATION

机译:低级煤热重整方法

摘要

PURPOSE:To reform coal having a low rank of coalification with high thermal efficiency into caking coal which hardly suffers spontaneous ignition, by adding pitch and water to coal having low rank of coalification to form a slurry, heat- treating the slurry under pressure and effecting heat exchange between the slurry after heating. CONSTITUTION:Coal having a low rank of coalification is crushed in a crusher 1. 0.02-2pts.wt. pitch such as coal tar and water or a mixture of water and an org. solvent such as toluene are added to one pt.wt. (on a dry basis) said coal and the mixture is mixed in a mixing tank 2 to form a slurry. The slurry is pressurized by a pressure pump 3, introduced through a heat exchanger 4 into a heating over 5 and heat-treated at 150-370 deg.C under pressure higher than saturated vapor pressure of water at that temp. to reform said coa. The treated slurry is fed to the heat exchanger 4 to make heat exchange between the slurry before heating and said slurry, and the resulting reformed coal is passed through an evaporator 7, a solid-liquid separator 9, etc. and recovered.
机译:目的:通过向低煤化等级的煤中添加沥青和水以形成浆液,在压力下对煤浆进行热处理并进行处理,从而将具有高热效率的低煤化等级的煤改造成几乎不会自燃的结块煤。加热后浆料之间的热交换。组成:具有低煤化等级的煤在1号破碎机中破碎。0.02-2pts.wt。沥青,例如煤焦油和水,或水和有机溶剂的混合物。将溶剂例如甲苯添加至1重量%。 (以干基计)所述煤和混合物在混合罐2中混合以形成淤浆。通过压力泵3对浆液加压,通过热交换器4将其引入加热装置5中,并在高于该温度下水的饱和蒸气压的压力下在150-370℃下进行热处理。改革说COA。将处理后的煤浆送入热交换器4,使加热前的煤浆与所述煤浆进行热交换,将生成的重整煤通过蒸发器7,固液分离器9等进行回收。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号