首页> 外国专利> PROCESS FOR THE PRODUCTION OF HIGH-GRADE COPPER BY PYROMETALLURGICAL REFINING OF BLISTER COPPER AND COPPER SCRAPS

PROCESS FOR THE PRODUCTION OF HIGH-GRADE COPPER BY PYROMETALLURGICAL REFINING OF BLISTER COPPER AND COPPER SCRAPS

机译:鼓泡铜和铜屑的高温冶金精炼生产高品位铜的方法

摘要

pA relatively simple and rapid process for the production of high-grade copper from an inexpensive starting material such as blister copper or copper scraps is described. The starting material is conventionally smelted and oxidized, after which the charge is subjected to a slagging operation to obtain a pre-refined copper bath. After the slagging step, an artificial slag cover is formed on the pre-refined copper bath using a mixture of (1) an oxide of at least one element selected from the group consisting of silicon, phosphorous and boron, and (2) an oxide of at least one element selected from the group consisting of titanium, aluminum, calcium, strontium, barium, magnesium, sodium, potassium and lithium. At least two of such elements are then fed to the bath through the slag cover as alloying components. After such resulting bath is mixed for at least 30 seconds and is left standing for an additional 15 minutes, the slag cover is removed. A conventional reduction step may then be accomplished to complete the refining process./p[US4055415A]
机译:描述了一种从廉价的起始材料例如泡铜或废铜生产高级铜的相对简单和快速的方法。常规上将原料熔化并氧化,然后对装料进行排渣操作以获得预精制的铜浴。在排渣步骤之后,使用(1)选自硅,磷和硼的至少一种元素的氧化物和(2)氧化物的混合物在预精炼的铜浴上形成人工渣盖。选自钛,铝,钙,锶,钡,镁,钠,钾和锂的至少一种元素。然后将至少两种这样的元素通过熔渣覆盖层作为合金成分送入熔池。将所得浴液混合至少30秒并静置15分钟后,将炉渣盖取下。然后可以完成常规的还原步骤以完成精炼过程。 [US4055415A]

著录项

  • 公开/公告号IN143749B

    专利类型

  • 公开/公告日1978-01-28

    原文格式PDF

  • 申请/专利权人 CSEPELI FEMMU;

    申请/专利号IN659CA1976

  • 发明设计人 DAROCZI SANDOR;NAGY TIBOR;STEFAN MIHALY;

    申请日1976-04-17

  • 分类号C22B9/12;C22B15/14;

  • 国家 IN

  • 入库时间 2022-08-22 22:48:52