首页> 外国专利> Method of producing normal grain growth (110) {8 001{9 {0 textured iron-cobalt alloys

Method of producing normal grain growth (110) {8 001{9 {0 textured iron-cobalt alloys

机译:产生正常晶粒长大的方法(110){8 001 {9 {0织构化的铁钴合金

摘要

An alloy and a method for producing the same are described in which the alloy is characterized by a primarily recrystallized microstructure having a (110) [001] orientation. The alloy contains from 5% to 35% cobalt, up to 2% chromium, up to 3% silicon, less than 0.005% sulfur and a balance essentially iron with incidental impurities. The method includes a schedule of hot and cold working the latter in limited amounts together with corresponding heat treatments producing the desired improved magnetic characteristics.
机译:描述了一种合金及其制造方法,其中该合金的特征在于具有(110)[001]取向的初次再结晶的微观结构。该合金包含5%至35%的钴,最多2%的铬,最多3%的硅,少于0.005%的硫和其余的基本上是铁以及附带的杂质。该方法包括以有限的数量对后者进行热和冷加工的时间表,以及产生所需改善的磁特性的相应热处理。

著录项

  • 公开/公告号US3892604A

    专利类型

  • 公开/公告日1975-07-01

    原文格式PDF

  • 申请/专利权人 WESTINGHOUSE ELECTRIC CORP.;

    申请/专利号US19740480075

  • 发明设计人 FOSTER;KARL;THORNBURG;DONALD R.;

    申请日1974-06-17

  • 分类号H01F1/00;

  • 国家 US

  • 入库时间 2022-08-23 03:29:00