Process comprises (a) oxidant preheating at 750-1300 degrees C of a seived graded charge e. iron bearing ores, sinter or pellets opt with fondants, (b) homogeneously mixing the preheated charge with a solid carbon reducing agent pref. cold seived coke, (c) introducing the total charge into =1 sealed vertical pretreatment furnace (I) which continuously feeds the electric furnace, (II), (d) lowering the charge in (I) in counter-current to hot reducing gases from (II) (e) injecting finely-divided air into the upper part of (I) to ensure neutral combustion of the gases which have somewhat prereduced the material in the lower part of (I), (f) evacuating and aspirating burnt gases so that the press of gases at the vault of (II) is constantly adjusted to a value close to that of the ambient atmos, and (g) injecting hydrocarbons opt. with O2 into the axis of Soderberg electrodes in (II) and close to their ends to obt. suitable qualities and quantities of reducing gases.
机译:该方法包括:(a)在750-1300℃下将分级的装料e预先氧化剂预热。铁粉矿石,烧结矿或球团矿与方旦糖一起选择,(b)将预热的装料与固体碳还原剂预混料均匀混合。冷筛分的焦炭,(c)将总装料引入> = 1的封闭式立式预处理炉(I)中,该炉连续供入电炉(II),(d)与热还原逆流降低(I)中的装料来自(II)的气体(e)将细分的空气注入(I)的上部,以确保中性燃烧的气体在某种程度上减少了(I)下部的材料,(f)排空并吸走已燃烧的气体气体,使(II)拱顶处的气体压力不断调整到接近周围大气的值,并且(g)选择注入烃。将氧气带入(II)中Soderberg电极的轴中,并靠近其末端。合适质量和数量的还原气体。

著录项

  • 公开/公告号FR2190922B1

    专利类型

  • 公开/公告日1974-10-25

    原文格式PDF

  • 申请/专利权人 CREUSOT LOIRE ENTREPRISEFR;

    申请/专利号FR19720024237

  • 发明设计人

    申请日1972-07-05

  • 分类号C21B13/00;

  • 国家 FR

  • 入库时间 2022-08-23 05:14:49

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号