首页> 外国专利> METHOD FOR MANUFACTURING DECK BOARD USING DOMESTICALLY PRODUCED OAK TREE AND DECK BOARD MANUFACTURED THEREBY

METHOD FOR MANUFACTURING DECK BOARD USING DOMESTICALLY PRODUCED OAK TREE AND DECK BOARD MANUFACTURED THEREBY

机译:使用国内生产的橡木树和甲板板制造甲板板的方法

摘要

The present invention relates to a method for manufacturing a domestic oak deck material in which the use of a domestic oak tree, in particular an oak thinning tree, as a high value-added product, and the splitting and distortion of the oak tree during drying are smoothly prevented so that the product is stably manufactured. , The present deck material manufacturing method comprises a step of preparing a wooden board (S10) of preparing a wooden board by cutting oak, and a step of installing a heating plate (S20) of forming a laminated wood by stacking the wooden board and a heating plate on the bogie, and the A drying chamber sealing step (S30) of inserting a bogie into the drying chamber and sealing the drying chamber, a vacuum forming step (S40) of forming a vacuum inside the drying chamber, and the forming of the vacuum into a shopping mall pressurizing plate. A vacuum pressurizing step (S50) of pressing the laminated wood, and a drying step (S60) of circulating hot water to the heating plate to dry the greenwood board to form a dry board, and the drying chamber during drying of the greenwood board. The pressing pressure control step (S70) of adjusting the pressing pressure by the pressing plate inside, the room temperature cooling step (S80) of circulating room temperature water to the heating plate through the room temperature cooling unit to cool the dried plate material (S80), and the drying plate material being heated to wood Including a plate material high heat treatment step (S90) to be put into the treatment device and treated with high heat.
机译:本发明涉及一种制造国产橡木甲板材料的方法,其中使用国内橡树,特别是橡木稀疏树作为高附加值的产品,以及在干燥过程中橡树树的分裂和变形平稳地防止,使产品稳定地制造。 ,本发明的甲板材料制造方法包括通过切割橡木制备制备木板的木板(S10)的步骤,以及通过堆叠木板和A的加热板(S20)安装加热板(S20)的步骤在转向架上的加热板,以及将转向架插入干燥室并密封干燥室的干燥室密封步骤(S30),在干燥室内形成真空的真空形成步骤(S40),以及形成真空吸入购物中心加压板。压制层压木材的真空加压步骤(S50),以及将热水循环到加热板的干燥步骤(S60),以使Greenwood板烘干,形成干燥的板,在干燥的Greenwood板期间干燥室。压制压力控制步骤(S70)通过压板通过压板调节压力,室温冷却步骤(S80)通过室温冷却单元向加热板循环室温水,冷却干燥的板材(S80 ),并且干燥板材料被加热到木材,包括板材高热处理步骤(S90)被放入治疗装置并用高热处理处理。

著录项

  • 公开/公告号KR102222941B1

    专利类型

  • 公开/公告日2021-03-04

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR1020190085372

  • 发明设计人 문중묵;

    申请日2019-07-15

  • 分类号B27M1/08;B27K5;B27M3/04;F26B7;

  • 国家 KR

  • 入库时间 2022-08-24 17:31:42