The present invention relates to a method of manufacturing seismic reinforcing bars with a yield strength of 620 MPa or higher, and to a seismic reinforcing bar with a yield strength of 620 MPa or higher produced by the manufacturing method. Produces seismic reinforcement with improved seismic performance by satisfying the yield ratio (YR; Yield Ratio) required by the company, and achieves a yield strength of 620 MPa or more by controlling the composition ratio of Mo (molybdenum) without adding expensive V (vanadium). At the same time, it satisfies the yield ratio (YR) required by KS to secure economic efficiency and reduce the production cost of seismic reinforcing bars.
机译:本发明涉及一种制造具有620MPa或更高的屈服强度的地震增强棒的方法,以及通过制造方法产生620MPa或更高的屈服强度的地震增强棒。通过满足公司所需的屈服比(Yr;屈服比),通过控制Mo(钼)的组成比,通过满足公司所需的屈服比(Yr;屈服比)来产生抗震性能的改善增强。在不添加昂贵的V(钒) 。同时,它满足KS所需的屈服比(YR),以确保经济效率,降低地震加强杆的生产成本。

著录项

  • 公开/公告号KR102252106B1

    专利类型

  • 公开/公告日2021-05-14

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR1020190101892

  • 发明设计人 이향준;

    申请日2019-08-20

  • 分类号C22C38/38;C21D8/08;C21D9;

  • 国家 KR

  • 入库时间 2022-08-24 18:48:22

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号