A nickel cobalt aluminum composite hydroxide, which is a precursor of a positive electrode active material, and which is composed of secondary particles to which primary particles containing a nickel, a cobalt, and an aluminum are aggregated, or composed of the primary particles and the secondary particles, wherein a sodium content contained in the nickel cobalt aluminum composite hydroxide is less than 0.0005% by mass. Also, a ratio of an average particle size of a lithium nickel cobalt aluminum composite oxide divided by an average particle size of the nickel cobalt aluminum composite hydroxide, which is a precursor, is 0.95 to 1.05, and further, when observing 100 or more particles of the lithium nickel cobalt aluminum composite oxide selected randomly by a scanning electron microscope, a number that an aggregation of secondary particles is observed is 5% or less with respect to a total number of observed secondary particles.
机译:氢钴铝复合氢氧化物,其是正极活性材料的前体,并且由次级颗粒组成,含有含有镍,钴和铝的初级颗粒的聚集,或由初级颗粒组成 二级颗粒,其中镍钴铝复合氢氧化物中含有的钠含量小于0.0005质量%。 而且,锂镍钴铝复合氧化物的平均粒径与镍钴铝复合氢氧化物的平均粒度的比例为0.95至1.05,并且在观察100或更多粒子时 通过扫描电子显微镜随机选择的锂镍钴铝复合氧化物,观察到二次颗粒的聚集的数量是相对于观察到的二次颗粒的总数为5%或更小。

著录项

  • 公开/公告号EP3916857A1

    专利类型

  • 公开/公告日2021-12-01

    原文格式PDF

  • 申请/专利权人 SUMITOMO METAL MINING CO. LTD.;

    申请/专利号EP20190911888

  • 发明设计人 OSHITA HIROKO;RYOSHI KAZUOMI;

    申请日2019-12-26

  • 分类号H01M4/525;

  • 国家 EP

  • 入库时间 2022-08-24 22:16:20

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号