Introducing crystallinity in polyimides offers the advantage of increased solvent resistance and retention of mechanical properties above the glass transition temperature(T_g). This work examines the thermal stability, semicrystalline morphology and adhesive properties of a new polyimide synthesized at Virginia Tech which is based on l,3-bis(4-aminophenoxy) benzene (TPER diamine) and 3,3',4,4'-biphenyltetracarboxylic dianhydride (BPDA). The polymer has a T_g of ca. 210°C and a T_m of 395°C. Polarized light microscopy was used to evaluate the morphology and spherulitic growth rates. The effects of molecular weight and melt conditions were studied in this regard. Lap-Shear specimens were made using Ti-6Al-4V alloy and the bonding conditions were optimized with respect to bonding temperature, bonding time and pressure. High lap-shear strengths of ca. 8000psi (55.172MPa) were obtained and the fracture surface investigation using the SEM revealed a very rough ductile surface. Durability studies on lap shears were conducted for aging and testing temperatures of ambient, 177°C and 232°C. Significant stability was observed for these aging temperatures for up to seven weeks. The bond strengths were found to be affected by testing temperatures rather than the aging conditions for the duration of the study. The effect of various solvents was investigated using lap-shear tests for periods up to 9 days.
机译:在聚酰亚胺中引入结晶度提供更高的耐溶剂性和高于玻璃化转变温度(T_G)机械性能的保留的优点。这项工作检查的热稳定性,半结晶形态和在弗吉尼亚技术合成的新聚酰亚胺,其是基于1,3-双(4-氨基苯氧基)苯(TPER二胺)和3,3' ,的粘合性能4,4'-联苯四甲酸二酐(BPDA)。的聚合物具有约的T_G 210℃和395℃的T_m。偏光显微镜来评价形态和球状的增长率。分子量和熔体条件的影响在这方面进行了研究。搭接剪切样品用的Ti-6Al-4V合金制成,并且接合条件相对于接合温度,接合时间和压力最优化。约的高搭接剪切强度8000psi(55.172MPa)获得并使用SEM的断裂面调查显示一个非常粗糙的表面延展的。上搭接剪切耐久性研究,老化和测试的环境的温度下进行,177℃和232℃。观察这些老化温度达七周显著稳定性。被发现的结合强度,以通过测试的温度,而不是老化条件的研究期间受到影响。使用周期9天搭接剪切测试各种溶剂的影响进行了研究。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号